  1. Ambient temperature mechanical properties for BS EN 10253-3 and 10253-4 for stainless steel butt weld fittings

    BS EN 10253-3 and 10253-4 are the EN standards for austenitic and duplex stainless steel butt-welding pipe fittings without and with specific inspection requirements. This article summarises the mechanical properties

  2. Ambient temperature mechanical properties of austenitic stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.

  3. Ambient temperature mechanical properties of austenitic stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic stainless steels.

  4. Ambient temperature mechanical properties of austenitic-ferritic (duplex) stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of austenitic-ferritic stainless steels.

  5. Ambient temperature mechanical properties of austenitic-ferritic (duplex) stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for austenitic-ferritic (duplex) stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given are proof strength, tensile strength, elongation and hardness.

  6. Ambient temperature mechanical properties of ferritic stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for ferritic stainless steel semi-finished products, bars, rods, wires, sections for general purposes. The current edition was published in October 2014. The properties given are proof strength, tensile strength, elongation and hardness for Bright Bars.

  7. Ambient temperature mechanical properties of ferritic stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for ferritic stainless steel semi-finished products, bars, rods, wires, sections for general purposes. The current edition was published in November 2014. The properties given are proof strength, tensile strength, elongation and hardness. LAST UPDATED 1st DECEMBER 2014.

  8. Ambient temperature mechanical properties of heat resisting steels to BS EN 10095

    BS EN 10095 is the material standard for heat resisting steels and nickel alloys. Mechanical properties (proof strength, tensile strength, hardness and elongation) of the common grades of stainless steel at ambient temperature covered in the standard are listed. Ferritic, austenitic and austenitic-ferritic (duplex) grades are included.

  9. Ambient temperature mechanical properties of martensitic and precipitation hardening stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of martensitic and precipitation hardening stainless steels.

  10. Ambient temperature mechanical properties of martensitic and precipitation hardening stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for martensitic and precipitation hardening stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given are proof strength, tensile strength, elongation and hardness.

Page 1 of 2

  1. 1
  2. 2

top

Office and Postal Address: BSSA, HQ, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital