  1. Ambient temperature mechanical properties of creep resisting steels to BS EN 10302

    BS EN 10302 is the recognised standard for creep resisting steels, nickel and cobalt alloys. This article summarises the mechanical properties for the steels listed in the standard.

  2. Ambient temperature mechanical properties of ferritic stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for ferritic stainless steel semi-finished products, bars, rods, wires, sections for general purposes. The current edition was published in October 2014. The properties given are proof strength, tensile strength, elongation and hardness for Bright Bars.

  3. Ambient temperature mechanical properties of ferritic stainless steel flat products to BS EN 10088-2

    The BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 2014. Mechanical properties are specified, including proof and tensile strength, and elongation. The tensile properties are tabulated in this article. LAST UPDATED 25th NOVEMBER 2014

  4. Ambient temperature mechanical properties of ferritic stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for ferritic stainless steel semi-finished products, bars, rods, wires, sections for general purposes. The current edition was published in November 2014. The properties given are proof strength, tensile strength, elongation and hardness. LAST UPDATED 1st DECEMBER 2014.

  5. Ambient temperature mechanical properties of heat resisting steels to BS EN 10095

    BS EN 10095 is the material standard for heat resisting steels and nickel alloys. Mechanical properties (proof strength, tensile strength, hardness and elongation) of the common grades of stainless steel at ambient temperature covered in the standard are listed. Ferritic, austenitic and austenitic-ferritic (duplex) grades are included.

  6. Ambient temperature mechanical properties of martensitic and precipitation hardening stainless steel bright bars to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given in this article are proof strength, tensile strength, elongation and hardness of martensitic and precipitation hardening stainless steels.

  7. Ambient temperature mechanical properties of martensitic and precipitation hardening stainless steel long products to BS EN 10088-3

    The BS EN 10088-3 standard gives the mechanical properties for martensitic and precipitation hardening stainless steel semi-finished products, bars, rods and sections for general purposes. The properties given are proof strength, tensile strength, elongation and hardness.

  8. Ambient temperature mechanical properties of martensitic stainless steel flat products to BS EN 10088-2

    The BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 2014. Mechanical properties are specified, including proof and tensile strength, elongation, impact strength and hardness. Only tensile and hardness properties are tabulated in this article for the martensitic grades. LAST UPDATED 25th NOVEMBER 2014.

  9. Ambient temperature mechanical properties of precipitation hardening stainless steel flat products to BS EN 10088-2

    The BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 2014. Mechanical properties are specified include proof strength, tensile strength and elongation. These are tabulated in this article for the precipitation hardening grades 1.4542 and 1.4568. LAST UPDATED 25th NOVEMBER 2014.

  10. Ambient temperature mechanical properties of stainless steels to BS EN 10269

    BS EN 10269 is the material standard for stainless and heat-resisting steels, a selection of low alloy steels and some nickel alloys for fasteners. The ambient temperature mechanical properties shown in this article include 0.2% proof strength, tensile strength, elongation, reduction in area and impact (charpy) strength in the finally heat treated condition. Specified hardness levels for the steels for subsequent quenching and tempering (1.4923 1.4938 and 1.4913) in their delivery condition are also included.

Page 2 of 6

  1. 1
  2. 2
  3. 3
  4. 4
  5. 5
  6. 6

top

Office and Postal Address: BSSA, Regus, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital