Stainless Steel Datasheets for Tubular Products

Introduction

The Stainless Steel Advisory Service receives requests for datasheets for individual steel grades. Rather than create a new set of datasheets, it has been decided to make use of the excellent datasheets which already exist. These datasheets are most often linked to BSSA Members. Occasionally, I have included a datasheet for grades which are not covered by Members' datasheets.

Steel grades are arranged according to the main EN standards for tubular products. The codes used in the following tables are:

Aalco Aalco
AM Aperam
DMV DMV
Out Outokumpu
RA Rolled Alloys
Sand Sandvik

The existence of a datasheet for the more unusual grades probably indicates the ability to supply. However, the Special Grades Matrix gives a more comprehensive list of companies able to supply the product.

 Datasheets for Welded Tubes Based on EN 10296-2 and EN 10217-7

The table below contains all grades listed in EN 10296-2 (welded tubes for general purposes) and EN 10217-7 (welded tubes for pressure purposes).  Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Grades in both standards are shown in bold. Grades only in EN 10296-2 are shown in normal. Grades only in EN 10217-7 are shown in italic.

EN Designation Alternative Designations  
Steel name Steel number AISI UNS Other US BS

Generic/Brand

Datasheets
Ferritic stainless steels
X2CrNi12 1.4003   S40977     3CR12 Aalco AM      
X2CrTi12 1.4512 409 S40900   409S19   AM      
X6CrAl13 1.4002 405 S40500   405S17          
X6Cr17 1.4016 430 S43000   430S17     AM      
X3CrTi17 1.4510 439 S43035         AM      
X2CrMoTi18-2 1.4521 444 S44400         AM      
X6CrMoNb17-1 1.4526 436 S43600         AM      
X2CrTiNb18 1.4509 441 S43932     18CrCb   AM      
Austenitic stainless steels
X2CrNiN18-7 1.4318 301LN S30153              
X2CrNi18-9 1.4307 304L S30403   304S11     AM      
X2CrNi19-11 1.4306 304L  S30403         AM      
X2CrNiN18-10 1.4311 304LN  S30453   304S51          
X5CrNi18-10 1.4301 304 S30400   304S15   AM      
X6CrNiTi18-10 1.4541 321  S32100   321S31     AM      
X6CrNiNb18-10 1.4550 347 S34700   347S31     -    
X2CrNiMo17-12-2 1.4404 316L  S31603   316S11     AM      
X5CrNiMo17-12-2 1.4401 316 S31600   316S31     AM      
X6CrNiMoTi17-12-2 1.4571 316Ti  S31635   320S31     AM      
X2CrNiMo17-12-3 1.4432 316L  S31603   316S13          
X2CrNiMoN17-3-3 1.4429 316LN S31653                
X3CrNiMo17-13-3 1.4436 316 S31600   316S33            
X2CrNiMo18-14-3 1.4435 316L  S31603   316S13          
X2CrNiMoN17-13-5 1.4439 317LMN S31726           But  
X1NiCrMoCu25-20-5 1.4539   N08904    904S13  904L   Outo    
X1CrNiMoCuN20-18-7 1.4547   S31254 F44   254SMO     Outo    
X6CrNiMoNb17-12-2 1.4580   S31640                
X2CrNiMo18-15-4 1.4438 317L S31703   317S12            
X1CrNiMoCuN24-22-8 1.4652   S32654     654SMO     Outo    
X1NiCrMo31-27-4 1.4563   N08028     Sanicro 28       But  
X1CrNiMoCuN25-25-5 1.4537   N08932                
X1CrNiMoCuNW24-22-6 1.4659   S31266                
X1NiCrMoCuN25-20-7 1.4529   N08925     1925hMo       But   
Austenitic stainless steels - heat resisting Grades
X15CrNiSi20-12 1.4828             AM    
X9CrNiSiNCe21-11-2 1.4835   S30815 253 MA   RA  
X12CrNi23-13 1.4833 309 S30900   309S24     AM   RA   
X8CrNi25-21 1.4845 310S S31000   310S24       RA  
X6CrNiSiNCe19-10 1.4818   S30415     153 MA     Outo    
X6NiCrSiNCe35-25 1.4854   S35315     353MA          
X10NiCrSi35-19 1.4886   N08330     330       RA  
Austenitic-ferritic stainless steels
X2CrMnNiN21-5-1 1.4162   S32101     2101 LDX     Outo    
X2CrNiN23-4 1.4362   S32304     2304     Outo    
X2CrNiMoN12-5-3 1.4462  

S31803/

S32205

 F51   2205   Outo RA  
X2CrNiMoN25-7-4 1.4410   S32750   F53   2507     Outo    
X2CrNiMoCuEWN25-7-4 1.4501 S32760 F55 Zeron 100 RA  

 

Datasheets for Seamless Tube Products Based on EN 10297-2 and EN 10216-5

The table below contains all grades listed in EN 10297-2 (seamless tubes for general purposes) and EN 10216-5 (seamless tubes for pressure purposes). Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Grades in both standards are shown in bold. Grades only in EN 10297-2 are shown in normal. Grades only in EN 10216-5 are shown in italic.

EN Designation Alternative designation
Steel name Steel number AISI UNS Other US BS Generic/Brand Datasheets
Ferritic stainless steels
X2CrTi12 1.4512 409 S40900   409S19            
X6CrAl13 1.4002 405 S40500   405S17        
X6Cr17 1.4016 430 S43000   430S17            
X3CrTi17 1.4510 439 S43035                
Martensitic stainless steels
X12Cr13 1.4006 410 S41000                
Austenitic stainless steels
X2CrNi18-9 1.4307 304L S30403   304S11            
X2CrNi19-11 1.4306 304L S30403                
X2CrNiN18-10 1.4311 304LN S30453                
X5CrNi18-10 1.4301 304 S30400   304S31            
X8CrNiS18-9 1.4305 303 S30300   303S31    

 

     
X6CrNiTi18-10 1.4541 321 S32100   321S31            
X6CrNiNb18-10 1.4550 347 S34700   347S31            
X1CrNi25-21 1.4335 310L S31002         Sand      
X2CrNiMo17-12-2 1.4404   S31603   316S11     

 

     
X5CrMo17-12-2 1.4401 316 S31600   316S31            
X1CrNiMoN25-22-2 1.4466 310MoLN S31050       DMV Sand      
X6CrNiMoTi17-12-2 1.4571 316Ti S31635   320S31            
X6CrNiMoNb17-12-2 1.4580   S31640                
X2CrNiMoN17-13-3 1.4429 316LN S31653                
X3CrNiMo17-13-3 1.4436 316 S31600   316S33          
X2CrNiMo18-14-3 1.4435 316L S31603       DMV Sand      
X2CrNiMoN17-13-5 1.4439   S31703                
X1NiCrMoCu31-27-4 1.4563   N08028     Sanicro 28   Sand      
X1NiCrMoCu25-20-5 1.4539   N08904     904L   Sand      
X1CrNiMoCuN20-18-7 4 1.4547   S31254     254 SMO   Sand      
X1NiCrMoCuN25-20-7 1.4529   N08925                
X2NiCrAlTi32-20 1.4558   N08800         Sand      
Ferritic heat resisting steels
X18CrN28 1.4749   S44600         Sand      
Austenitic heat resisting steels
X8CrNiTi18-10 1.4878 321 S32109                
X9CrNiSiNCe21-11-2 1.4835   S30815     253 MA   Sand      
X12CrNi23-13 1.4833   S30900   309S24     Sand      
X8CrNi25-21 1.4845 310S S31008   310S31     Sand      
X10NiCrAlTi32-21 1.4876   N08810                
X6NiCrSiNCe35-25 1.4854   S35315         Sand      
X10NiCrSi35-19 1.4886   N08330     330     RA    
 Austenitic creep resisting steels
X6CrNi18-10 1.4948 304H                  
X7CrNiTi18-10 1.4940 321H                  
X7CrNiNb18-10 1.4912 347H                  
X6CrNiTiB18-10 1.4941 321H                  
X6CrNiMo17-13-2 1.4918 316N           Sand      
X5NiCrAlT31-20 1.4958                    
X8CrNiAlTi32-21 1.4959             Sand      
X3CrNiMoBN17-13-3 1.4910 316LN                  
X8CrNiNb16-13 1.4961                    
X8CrNiMoVNb16-13 1.4988                    
X8CrNiMoNb16-16 1.4981                    
X10CrNiMoMnNbVB15-10-1 1.4982             Sand      
Austenitic-ferritic stainless steels
X2CrNiN23-4 1.4362   S32304     2304   Sand      
X3CrNiMoN27-5-2 1.4460 329 S31260         Sand      
X2CrNiMoN29-7-2 4 1.4477                    
X2CrNiMoN22-5-3 1.4462  

S31803/

S32205

    2205 DMV Sand      
X2CrNiMoCuN25-6-3 1.4507   S32550     Ferrinox 255 DMV        
X2CrNiMoN25-7-4 4 1.4410   S32750     2507   Sand    
X2CrNiMoCuWN25-7-4 1.4501   S32760     Zeron 100 DMV        
X2CrNiMoSi18-5-3 1.4424   S31500         Sand      

top

Office and Postal Address: BSSA, Regus, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital