Availability of Stainless Steel Grades

Availability of Stainless Steel Products

The tables below give an indication of the availability of stainless steel flat and long products. The intention is to give designers and specifiers some idea of how easy it will be to source their choice of grade and product form. The information has been created as a response to enquiries for rare grades which are difficult to source in small quantities.

Comments are invited on the tables. It is likely with such a large amount of information that there are some differences of opinion about the availability of some grades. If you want to make a comment on this table please email to ssas@bssa.org.uk.

Availability of Flat Products Grades from EN 10088-2

The table below contains all grades listed in EN 10088-2. The meaning of the availability scores is:

1 - Readily available from any recognised stainless steel stockholder

2 - Available from a significant number of specialist stainless steel stockholders

3 - Available from a limited number of suppliers

4 - Available only from stainless steel mills if sufficient quantity required

5 - Not practically available

N/A - Not applicable - Indicates that the grade is not intended to be made in that product form. For example, most ferritic grades would not be made as plate.

EN Designation Alternative Designations  Availability
Steel name Steel number AISI UNS Other US BS

Generic/Brand

Plate Sheet
Ferritic stainless steels - standard grades
X2CrNi12 1.4003   S40977     3CR12 2 2
X2CrTi12 1.4512 409 S40900   409S19   N/A 2
X6CrNiTi12 1.4516           N/A
X6Cr13 1.4000 410S S41008   403S17   3
X6CrAl13 1.4002 405 S40500   405S17   4 4
X6Cr17 1.4016 430 S43000   430S17   N/A 1
X3CrTi17 1.4510 439 S43035       N/A 2
X3CrNb17 1.4511 430Nb         N/A 4
X6CrMo17-1 1.4113 434 S43400   434S17   N/A 4
X2CrMoTi18-2 1.4521 444 S44400       N/A 3
Ferritic stainless steels - special grades
X2CrTi17 1.4520           N/A 4
X1CrNb15 1.4595           N/A 4
X2CrMoTi17-1 1.4513           N/A 4
X6CrNi17-1 1.4017           N/A 4
X5CrNiMoTi15-2 1.4589   S42035       N/A 4
X6CrMoNb17-1 1.4526 436 S43600       N/A 3
X2CrNbZr17 1.4590           N/A 4
X2CrTiNb18 1.4509 441 S43932     18CrCb N/A 2
X2CrMoTi29-4 1.4592   S44700     29-4  N/A 4
X2CrMnNiTi12 1.4600           N/A 3
X2CrSiTi15 1.4630           N/A 3
X2CrAlSiNb18 1.4634           N/A 3
X2CrNbTi20 1.4607           N/A 3
X2CrTi21 1.4611           N/A 3
X2CrNbCu21 1.4621           N/A 3
X2CrTi24 1.4613           N/A 3
Ferritic stainless steels - heat resisting grades
X10CrAlSi7 1.4713           3 3
X10CrAlSi13 1.4724           3 3
X10CrAlSi18 1.4742           3 3
X18CrN28 1.4749 446         3 3
X10CrAlSi25 1.4762           3 3
Martensitic stainless steels - standard grades
X12Cr13 1.4006 410  S41000   410S21   3 3
X15Cr13 1.4024 420  S42000       3 3
X20Cr13 1.4021 420 S42000   420S29   3 3
X30Cr13 1.4028 420 S42000   420S45   3 3
X39Cr13 1.4031 420 S42000   420S45   3 3
X46Cr13 1.4034 420 S42000        3 3
X38CrMo14 1.4419           5 5
X55CrMo14 1.4110           5 5
X50CrMoV15 1.4116           4 4
X39CrMo17-1 1.4122           5 5
X3CrNiMo13-4 1.4313   S41500 F6NM     3 3
X4CrNiMo16-5-1 1.4418         248 SV 3 3
Martensitic and precipitation-hardening steels - special grades
X1CrNiMoCu12-5-2 1.4422           5 5
X1CrNiMoCu12-7-3 1.4423           5 5
X5CrNiCuNb16-4 1.4542   S17400     17-4 PH 3 3
X7CrNiAl17-7 1.4568   S17700     17-7 PH N/A  2
Austenitic stainless steels - standard grades
X10CrNi18-8 1.4310 301  S30100   301S21   N/A 2
X2CrNiN18-7 1.4318 301LN S30153       N/A 3
X2CrNi18-9 1.4307 304L S30403   304S11   1 1
X2CrNi19-11 1.4306 304L  S30403       4 4
X2CrNiN18-10 1.4311 304LN  S30453   304S51   3 4
X5CrNi18-10 1.4301 304 S30400   304S15   1 1
X8CrNiS18-9 1.4305 303  S30300   303S31   3 N/A
X6CrNiTi18-10 1.4541 321  S32100   321S31   2 2
X4CrNi18-12 1.4303 305  S30500   305S19   N/A 4
X2CrNiMo17-12-2 1.4404 316L  S31603   316S11   1 1
X2CrNiMoN17-11-2 1.4406 316LN  S31653   316S61   4 4
X5CrNiMo17-12-2 1.4401 316 S31600   316S31   1 1
X6CrNiMoTi17-12-2 1.4571 316Ti  S31635   320S31   3 3
X2CrNiMo17-12-3 1.4432 316L  S31603   316S13   2 3
X2CrNiMo18-14-3 1.4435 316L  S31603   316S13   4 4
X2CrNiMoN17-13-5 1.4439 317LMN         4 4
X1NiCrMoCu25-20-5 1.4539   N08904    904S13  904L 3 3
Austenitic stainless steels - special grades
X5CrNi17-7 1.4319           4 4
X5CrNiN19-9 1.4315           4 4
X1CrNi25-21 1.4335 310L         4 4
X6CrNiNb18-10 1.4550 347 S34700   347S31   4 3
X1CrNiMoN25-22-2 1.4466 310MoLN S31050       4 4
X6CrNiMoNb17-12-2 1.4580           5 5
X2CrNiMoN17-3-3 1.4429 316LN S31653       4 4
X3CrNiMo17-13-3 1.4436 316 S31600   316S33   3 3
X2CrNiMoN18-12-4 1.4434 317LN  S31753       4 4
X2CrNiMo18-15-4 1.4438 317L     317S12   4 4
X1CrNiMoCuN24-22-8 1.4652           4 4
X1CrNiSi18-15-4 1.4361           4
X11CrNiMnN19-8-6 1.4369           4 3
X12CrMnNiN17-7-5 1.4372 201 S20100        4 3
X2CrMnNiN17-7-5 1.4371 201L S20103        4 3
X12CrMnNiN18-9-5 1.4373 202 S20200       4 3
X9CrMnCuNB17-8-3 1.4597 204Cu S20430       N/A 3
X1NiCrMo31-27-4 1.4563   N08028     Sanicro 28
X1CrNiMoCuN25-25-5 1.4537           5 5
X1CrNiMoCuN20-18-7 1.4547   S31254  F44   254SMO
X1CrNiMoCuNW24-22-6 1.4659          
X1NiCrMoCuN25-20-7 1.4529   N08925     1925hMo 3
X2CrNiMnMoN25-18-6-5 1.4565           N/A
X9CrMnNiCu 17-8-5-2 1.4618           N/A 3
X2CrNiMnMoNNb21-16-5-3 1.3964         XM-19 3 N/A
X8CrMnNi19–6-3 1.4376           3 3
X5CrNiCu19–6-2 1.4640           3 3
X6CrMnNiCuN18–12–4-2 1.4646           3 3
Austenitic stainless steels - heat resisting grades
X8CrNiTi18-10 1.4878 321 S32100       3
X15CrNiSi20-12 1.4828           3
X9CrNiSiNCe21-11-2 1.4835   S30815     253 MA 3 3
X12CrNi23-13 1.4833 309 S30900   309S24   3 3
X8CrNi25-21 1.4845 310S S31000   310S24   2
X15CrNiSi25-21 1.4841 314 S31400       4 4
X6CrNiSiNCe19-10 1.4818   S30415     153 MA
X10NiCrSi35-19 1.4886         330
Austenitic stainless steels - creep resisting grades
X6CrNi18-10 1.4948 304H S30409   304S51   3
X6CrNiMoB17-12-2 1.4919 316H S31635   316S51   4
Austenitic-ferritic stainless steels-standard grades
X2CrNiN22-2 1.4062   S32202     DX 2202 3 3
X2CrMnNiN21-5-1 1.4162   S32101     2101 LDX
X2CrNiN23-4 1.4362   S32304     2304
X2CrNiMnMoCuN24–4-3–2 1.4662         2404 LDX 3 3
X2CrMnNiMoN21–5-3 1.4482           3 3
X2CrNiMoN12-5-3 1.4462  

S31803/

S32205

 F51   2205 2 2
Austenitic-ferritic stainless steels-special grades
X2CrNiCuN23-4 1.4655           5
X2CrNiMoN29-7-2 1.4477           5
X2CrNiMoCuN25-6-3 1.4507      F61   Ferrinox 255
X2CrNiMoN25-7-4 1.4410   S32750   F53   2507
X2CrNiMoCuWN25-7-4 1.4501   S32760  F55   Zeron 100 2 3
X2CrNiMoSi18-5-3 1.4424           5 5

 

Availability of Long Products Grades from EN 10088-3


The table below contains all grades listed in EN 10088-3. The meaning of the availability scores is:

1 - Readily available from any recognised stainless steel stockholder

2 - Available from a significant number of specialist stainless steel stockholders

3 - Available from a limited number of suppliers

4 - Available only from stainless steel mills if sufficient quantity required

5 - Not practically available

N/A - Not applicable - Indicates that the grade is not intended to be made in that product form. For example, most ferritic grades would not be made as plate.

 

The table below contains all grades listed in EN 10088-3. In addition, there are some grades not in the current edition but which are expected to be in future editions. Some heat resisting steels from EN 10095 and creep resisting steels from EN 10302 are also included.

EN Designation  Alternative designation Availability
Steel name Steel number AISI UNS Other US BS Generic/Brand Bar Wire
Ferritic stainless steels-standard grades
X2CrNi12 1.4003   S40977       3 4
X6Cr13 1.4000 410S S41008   403S17   3 3
X6Cr17 1.4016 430 S43000   430S17   2 2
X6CrMoS17 1.4105           2
X6CrMo17-1 1.4113 434 S43400        3
Ferritic stainless steels-special grades
X2CrTi17 1.4520           4
X3CrNb17 1.4511           4 4
X2CrMoTiS18-2 4 1.4523           4 4
X6CrMoNb17-1 1.4526 436 S43600       4 4
X2CrTiNb18 1.4509 441 S43932     18CrCb 4 4
X2CrTi21 1.4611           3 3
X2CrNbCu21 1.4621           3 3
X2CrTi24 1.4613           3 3
Ferritic stainless stees - Heat resisting grades
X10CrAlSi7 1.4713           3 3
X10CrAlSi18 1.4742           4 4
X10CrAlSi25 1.4762           4 4
Martensitic stainless steels-standard grades
X12Cr13 1.4006 410 S41000       2 2
X12CrS13 1.4005 416 S41600       2 2
X20Cr13 1.4021 420 S42000   420S29   2 2
X30Cr13 1.4028 420 S42000   420S45   2 2
X39Cr13 1.4031 420 S42000   420S45   3
X46Cr13 1.4034 420 S42000       3 3
X38CrMo14 1.4419           4 4
X50CrMoV15 1.4116           3 3
X55CrMo14 1.4110           4 4
X14CrMoS17 1.4104           2 2
X39CrMo17-1 1.4122           2 N/A
X17CrNi16-2 1.4057 431 S43100   431S29   1 N/A
X3CrNiMo13-4 1.4313   S41500 F6NM     3 N/A
X4CrNiMo16-5-1 1.4418         248SV 3 N/A
Martensitic stainless steels-special grades
X29CrS13 1.4029           4
X46CrS13 1.4035           4 4
X70CrMo15 1.4109           3
X40CrMoVN16-2 1.4123           4 4
X105CrMo17 1.4125 440C S44004       3 N/A
X90CrMoV18 1.4112 440B S44003       3 N/A
X2CrNiMoV13-5-2 1.4415           4 4
X53CrSiMoVN16-2 1.4150           3 3
Martensitic stainless steels-creep resisting grades
X20CrMoV11-1 1.4922           3 N/A
X22CrMoV12-1 1.4923           3 N/A
Precipitation hardening stainless steels-standard grades
X5CrNiCuNb16-4 1.4542   S17400     17-4 PH 2 3
X7CrNiAl17-7 1.4568   S17700     17-7 PH N/A
X5CrNiMoCuNb14-5 1.4594         FV 520B 3 N/A
Precipitation hardening stainless steels-special grades
X1CrNiMoAlTi12-9-2 1.4530           4 N/A
X1CrNiMoAlTi12-10-2 1.4596           4 N/A
X5NiCrTiMoVB25-12-2 1.4606           N/A
X1CrNiMoAlTi12-11-2 1.4612           3 3
Austenitic stainless steels-standard grades
X10CrNi18-8 1.4310 301 S30100   301S21   N/A
X2CrNi18-9 1.4307 304L S30403   304S11   1 1
X2CrNi19-11 1.4306 304L S30403   304S11    3 3
X2CrNiN18-10 1.4311 304LN S30453   304S61   3
X5CrNi18-10 1.4301 304 S30400   304S31   1 1
X8CrNiS18-9 1.4305 303 S30300   303S31   1 1
X6CrNiTi18-10 1.4541 321 S32100   321S31   2 2
X4CrNi18-12 1.4303 305 S30500       4 4
X2CrNiMo17-12-2 1.4404   S31603   316S11   1 1
X2CrNiMoN17-11-2 1.4406 316LN S31653       4
X5CrMo17-12-2 1.4401 316 S31600   316S31   1 1
X6CrNiMoTi17-12-2 1.4571 316Ti S31635    320S31   2 2
X2CrNiMo17-12-3 1.4432 316L S31603    316S13   4
X2CrNiMoN17-13-3 1.4429 316LN S31653        3 4
X3CrNiMo17-13-3 1.4436 316 S31600    316S33   3 3
X2CrNiMo18-14-3 1.4435 316L S31603        3 3
X2CrNiMoN17-13-5 1.4439 317LMN S31726        4
X6CrNiCuS18-9-2 1.4570           3 3
X3CrNiCu18-9-4 1.4567 304Cu S30430    394S17    2 2
X1NiCrMoCu25-20-5 1.4539 904L N09804    904S13    2 2
Austenitic stainless steels-special grades
X5CrNi17-7 1.4319 302  S30200    302S25    2
X9CrNi18-9 1.4325          
X5CrNiN19-9 1.4315 304N  S30451        4
X6CrNiNb18-10 1.4550 347 S34700    347S31   3 4
X1CrNiMoN25-22-2 1.4466 310MoLN S31050       4
X6CrNiMoNb17-12-2 1.4580 316Cb  S31640       
X2CrNiMo18-15-4 1.4438 317L S31703    317S12   4
X1CrNiMoCuN24-22-8 1.4652 S32654        654SMO
X1CrNiSi18-15-4 1.4361 306  S30600       
X11CrNiMnN19-8-6 1.4369          
X12CrMnNiN17-7-5 1.4372 201 S20100       3
X8CrMnNiN18-9-5 1.4374           4
X8CrMnCuNB17-8-3 1.4597 S20430          3
X3CrNiCu19-9-2 1.4560           4
X3CrNiCuMo17-11-3-2 1.4578           4
X1NiCrMoCu31-27-4 1.4563   N08028      Sanicro 28 3
X1CrNiMoCuN25-25-5 1.4537   N08932        4
X1CrNiMoCuN20-18-7 4 1.4547   S31254     254 SMO 3
X2CrNiMoCuS17-10-2 1.4598           3
X1CrNiMoCuNW24-22-6 1.4659    S31266       4
X1NiCrMoCuN25-20-7 1.4529   N08925      1925hMo 3
X2CrNiMnMoN25-18-6-5 1.4565   S34565        3 4
X2CrNiMnmoNNb21-16-5-3 1.3964   S20910     Nitronic 50 3
      S21800     Nitronic 60
X3CrMnNiCu15-8-5-3 1.4615           3 3
X13MnNiN18-13-2 1.4020           3 3
X6CrMnNiN18-3-3 1.4378           3 3
X6CrMnNiCuN18-12-4-2 1.4646           3 3
Austenitic stainless steels - Heat resisting steels
X6CrNiSiNCe19-10 1.4818   S30415       4
X15CrNiSi20-12 1.4828 309Si         3 3
X12CrNi23-13 1.4833 309  S30900    309S16    3 3
X9CrNiSiNCe21-11-2 1.4835   S30815     253 MA 3 3
X8CrNi25-21 1.4845 310S S31008   310S31   2 2
X15CrNiSi25-21 1.4841 314 S31400       2
X12NiCrSi35-16 1.4864           4 3
X10NiCrSi35-19 1.4886 330 N08330        3 3
Austenitic stainless steels - Creep resisting grades
X6CrNiMoB17-12-2 1.4919 316H S31609       4 4
X6CrNi18-10 1.4948 304H S30409        3 3
X6NiCrTiMoVB25-15-2 1.4980   S66286     A286  3 4
Austenitic-ferritic stainless steels-Standard grades
X2CrNiN22-2 1.4062   S32202     DX 2202 3 3
X2CrMnNiN21-5-1 1.4162   S32101     2101 LDX 2
X3CrNiMoN27-5-2 1.4460 329 S31260       3 N/A 
X2CrNiMoN22-5-3 1.4462  

S31803/

S32205

    2205 2 2
Austenitic-ferritic stainless steels-special grades
X2CrNiN23-4 1.4362   S32304     2304 3
X2CrNiMoN29-7-2 4 1.4477           4
X2CrNiMoCuN25-6-3 1.4507   S32550     Ferrinox 255 2 2
X2CrNiMoN25-7-4 4 1.4410   S32750     2507 2
X2CrNiMoCuWN25-7-4 1.4501   S32760     Zeron 100 2
X2CrNiMoSi18-5-3 1.4424   S31500       4
X2CrMnNiMoN21-5-3 1.4482           3 3
X2CrNiMnMoCuN24-4-3-2 1.4662         2404 LDX 3 3
X2CrCuNiN23-2-2 1.4669           3 3

top

Office and Postal Address: BSSA, HQ, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital