British and american standards for tolerances, surface finish and testing of stainless steels

Introduction

The table shows both current and obsolete standards (where these may be of current interest) in the 'Status' column. 'C' is current, 'W' is withdrawn, "S" is superseded for stainless steels, that is the standard was applicable to all steels but there is now a new standard covering stainless steels only.
The 'date' is the current publication year.
Use the 'Ctrl' and 'F' keys to 'find' the standard you are looking for.

These lists cannot be guaranteed as complete and accurate by the BSSA.
In cases of doubt the catalogues maintained by the British Standards Institution should be used.

Table

Std Number Date Status Title
Tolerances and surfaces
BS EN ISO 1127 1997 C Stainless Steel Tubes - Dimensions, Tolerances and Conventional Masses Per Unit Length
BS EN ISO 9444-1 2009 C Continuously hot-rolled stainless steel - Tolerances on dimensions and form . Part 1: Narrow strip and cut lengths
BS EN ISO 9444-2 2010 C Continuously hot-rolled stainless steel. Tolerances on dimensions and form. Wide strip and sheet/plate
BS EN ISO 9445-1 2010 C Continuously cold-rolled stainless steel. Tolerances on dimensions and form. Narrow strip and cut lengths
BS EN ISO 9445-2 2010 C Continuously cold-rolled stainless steel. Tolerances on dimensions and form. Wide strip and plate/sheet
BS EN 10029 1991 S Tolerances on Dimensions, Shape and Mass for Hot Rolled Steel Plates 3mm Thick or Above. Replaced by BS EN ISO 18286
BS EN 10048 1997 Hot Rolled Narrow Steel Strip - Tolerances on Dimensions and Shape. Replaced by BS EN ISO 9444-1
BS EN 10051 2010 Continuously Hot-Rolled Uncoated Plate, Sheet and Strip of Non-Alloy and Alloy Steels - Tolerances on Dimensions and Shape. Replaced by BS EN ISO 9444-2
BS EN 10058 2003 C Hot Rolled Flat Steel Bars for General Purposes - Dimensions and Tolerances on Shape and Dimensions
BS EN 10059 2003 C Hot Rolled Square Steel Bars for General Purposes - Dimensions and Tolerances on Shape and Dimensions
BS EN 10060 2003 C Hot Rolled Round Steel Bars for General Purposes - Dimensions and Tolerances on Shape and Dimensions
BS EN 10061 2003 C Hot Rolled Hexagon Steel Bars for General Purposes - Dimensions and Tolerances on Shape and Dimensions
BS EN 10258 1997 Cold Rolled Stainless Steel Narrow Strip and Cut Lengths - Tolerances on Dimensions and Shape. Replaced by BS EN ISO 9445-1
BS EN 10259 1997 W Cold Rolled Stainless Steel Wide Strip and Plate/Sheet Tolerances on Dimensions and Shape. Replaced by BS EN ISO 9445-2
BS EN 10278 1999 C Dimensions and Tolerances of Bright Steel Products
BS EN ISO 18286 2010 C Hot-rolled stainless steel plates. Tolerances on dimensions and shape
BS 1134-1 1988 C Assessment of Surface Texture-Methods & Instrumentation
Passivation and cleaning
BS EN 2516 1997 C Passivation of Corrosion Resisting Steels and Decontamination of Nickel Base Alloys
BS ISO 15730 2000 C Metallic and other Inorganic Coatings. Electropolishing as a Means of Smoothing and Passivating Stainless Steel
 
ASTM A380 - - Practice for Cleaning, Descaling and Passivation of Stainless Steel Parts, Equipment and Systems
ASTMA380 ASTM A967 - - Specification for Chemical Passivation Treatments for Stainless Steel Parts
Testing
BSEN 10204 2004 C Metallic Products - Types of Inspection Documents
BSEN 10228-4 1999 C Non-Destructive Testing of Steel Forgings. Ultrasonic Testing of Austenitic and Austenitic-Ferritic Stainless Steel Forgings
BSEN 10307 2001 C Non-destructive testing. Ultrasonic testing of austenitic and austentitic-ferritic stainless steels flat products of thickness equal to or greater than 6 mm (reflection method)
BSENISO 3651 1998 C Determination of Resistance to Intergranular Corrosion of Stainless Steels
BSISO 11408 1999 C Chemical Conversion Coatings - Black Oxide Coating on Iron and Steel - Specification and Test Methods
BSISO 16701 2003 C Corrosion of Metals and Alloys-Corrosion in Artificial Atmosphere-Accelerated Corrosion Test Involving Exposure Under Controlled Conditions of Humidity Cycling and Intermittent Spraying of a Salt Solution

top

Office and Postal Address: BSSA, Regus, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital