British standards for the welding and fabrication of stainless steels

Introduction

The table shows both current and obsolete standards (where these may be of current interest) in the 'Status' column. 'C' is current and 'W' is withdrawn.
The 'date' is the original publication year.
Use the 'Ctrl' and 'F' keys to 'find' the standard you are looking for.

These lists cannot be guaranteed as complete and accurate by the BSSA.
In cases of doubt the catalogues maintained by the British Standards Institution should be used.

Table

Std Number Date Status Title
BS 2633 1987 C Specification for Class I Arc Welding of Ferritic Steel Pipework for Carrying Fluids
BS 4677 1984 C Specification for Arc Welding of Austenitic Stainless Steel Pipework for Carrying Fluids
BS 4515-2 1999 C Specification for Welding of Steel Pipelines on Land And Offshore - Duplex Stainless Steel Pipelines
BS 7475 1991 W Specification for Fusion Welding of Austenitic Stainless Steels
BS EN 1011-3 2000 C Welding-Recommendtaions for Welding of Metallic Materials - Part 3: Arc Welding of Stainless Steels
BS EN 1600 1997 C Covered Electrodes for Manual Metal Arc Welding of Stainless and Heat Resisting Steels
BS EN 12072 2000 C Welding Consumables-Wire Electrodes, Wires and Rods for Arc Welding of Stainless and Heat-Resisting Steels - Classification
BS EN 12073 2000 W Tubular cored electrodes for metal arc welding, with or without a gas shield, of stainless and heat resisting steels - Classification.
BS EN ISO 17633 2010 C Tubular cored electrodes and rods for gas shielded and non-gas shielded metal arc welding of stainless and heat-resisting steels
BS EN 760 1996 C Welding Consumables-Fluxes for Submerged Arc Welding - Classification
BS EN 287-1 2011  C Qualification test of welders. Fusion welding. Steels 
 
BS EN 288

 

1992

1992

1992

1995

1995   

C Specification and Approval of welding Procedures for Metallic Materials
Part 1. Welding Procedure Tests for the Arc Welding of Steels
Part 2. Welding Procedure Specification for Arc Welding
Part 3. Welding Procedure Tests for the Arc Welding of Steels
Part 5. Approval by Using Approved Welding Consumables for Arc Welding
Part 6. Approval Related to Previous Experience
Part 7. Approval by a Standard Welding Procedure for Arc Welding
BS 6787 1989 C Method for Determination of Ferrite Number in Austenitic Weld Metal Deposited by Covered Cr-Ni Steel Electrodes
BS 5245 1975 C Specification for Phosphoric Acid Based Flux for Soft Soldered Joints in Stainless Steel
BS EN ISO 3506 2009  C Mechanical Properties of Corrosion Resistant Stainless Steel Fasteners
BS 6105 1981 W Specification for Corrosion Resistant Fasteners
BS 1210 1963 C Specification for Wood Screws

top

Office and Postal Address: BSSA, Regus, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital