Stainless Steel Grades Datasheets

Introduction

The Stainless Steel Advisory Service receives requests for datasheets for individual steel grades. Rather than create a new set of datasheets, it has been decided to make use of the excellent datasheets which already exist. These datasheets are most often linked to BSSA Members. Occasionally, we have included a datasheet for grades which are not covered by Members' datasheets.

Steel grades are arranged according to the main EN standards for flat and long products.

The codes used in the following tables are:

Ace Acerinox
AK AK Steel
AP Aperam
NN NeoNickel
Out Outokumpu
Sm Smith Metal Centres
Val Valbruna

The existence of a datasheet for the more unusual grades probably indicates the ability to supply. However, the Special Grades Matrix gives a more comprehensive list of companies able to supply the product.

 Datasheets for Flat Products Based on EN 10088-2

The table below contains all grades listed in EN 10088-2. In addition, there are some grades not in the current edition but which are expected to be in future editions. Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Some heat resisting steels from EN 10095 and creep resisting steels from EN 10302 are also included.

EN Designation

Alternative Designations

 

Steel name

Steel number

AISI

UNS

Other US

BS

Generic/ Brand

Datasheets

Ferritic stainless steels - standard grades

X2CrNi12

1.4003

 

S40977

 

 

3CR12

ACE

 

AP

OUT

 

X2CrTi12

1.4512

409

S40900

 

409S19

 

ACE

AK

AP

OUT

 

X6CrNiTi12

1.4516

 

 

 

 

 

 

 

 

 

 

X6Cr13

1.4000

410S

S41008

 

403S17

 

 

AK

 

 

 

X6CrAl13

1.4002

405

S40500

 

405S17

 

 

 

 

 

 

X6Cr17

1.4016

430

S43000

 

430S17

 

ACE

AK

AP

OUT

 

X3CrTi17

1.4510

439

S43035

 

 

 

ACE

AK

AP

OUT

 

X3CrNb17

1.4511

430Nb

 

 

 

 

ACE

AK

 

 

 

X6CrMo17-1

1.4113

434

S43400

 

434S17

 

ACE

 

 

 

 

X2CrMoTi18-2

1.4521

444

S44400

 

 

 

ACE

AK

AP

OUT

 

Ferritic stainless steels - special grades

X2CrMnTi12

1.4600

 

 

 

 

 

 

 

 

 

 

X2CrSiTi15

1.4630

 

 

 

 

 

 

 

 

 

 

X2CrTi17

1.4520

 

 

 

 

 

 

 

 

 

 

X1CrNb15

1.4595

 

 

 

 

 

 

 

 

 

 

X2CrMoTi17-1

1.4513

 

 

 

 

 

 

 

AP

 

 

X6CrNi17-1

1.4017

 

 

 

 

 

 

 

 

 

 

X5CrNiMoTi15-2

1.4589

 

S42035

 

 

 

 

 

 

 

 

X6CrMoNb17-1

1.4526

436

S43600

 

 

 

ACE

AK

AP

 

 

X2CrNbZr17

1.4590

 

 

 

 

 

 

 

 

 

 

X2CrTiNb18

1.4509

441

S43932

 

 

18CrCb

ACE

AK

AP

OUT

 

X2CrNbTi20

1.4607

 

 

 

 

 

 

 

 

 

 

X2CrTi21

1.4611

 

 

 

 

 

 

 

 

 

 

X2CrTi24

1.4613

 

 

 

 

 

 

 

 

 

 

X2CrMoTi29-4

1.4592

 

S44700

 

 

29-4

 

 

 

 

 

X2CrNbCu21

1.4621

 

S44500

 

 

 

 

 

AP

 

 

X2CrTiNbVCu22

1.4622

 

S44330

 

 

 

 

 

 

OUT

 

Ferritic stainless steels - heat resisting grades

X10CrAlSi7

1.4713

 

 

 

 

 

 

 

 

OUT

 

X10CrAlSi13

1.4724

 

 

 

 

 

 

 

 

OUT

 

X10CrAlSi18

1.4742

 

 

 

 

 

 

 

 

OUT

 

X18CrN28

1.4749

446

 

 

 

 

 

 

 

 

 

X10CrAlSi25

1.4762

 

 

 

 

 

 

 

 

OUT

 

Martensitic stainless steels - standard grades

X12Cr13

1.4006

410

S41000

 

410S21

 

 

 

 

 

 

X15Cr13

1.4024

420

S42000

 

 

 

 

 

 

 

 

X20Cr13

1.4021

420

S42000

 

420S29

 

 

 

AP

 

 

X30Cr13

1.4028

420

S42000

 

420S45

 

 

 

AP

 

 

X39Cr13

1.4031

420

S42000

 

420S45

 

ACE

 

 

 

 

X46Cr13

1.4034

420

S42000

 

 

 

 

 

AP

 

 

X38CrMo14

1.4419

 

 

 

 

 

 

 

AP

 

 

X55CrMo14

1.4110

 

 

 

 

 

 

 

 

 

 

X50CrMoV15

1.4116

 

 

 

 

 

ACE

 

 

 

 

X39CrMo17-1

1.4122

 

 

 

 

 

 

 

 

 

 

X3CrNiMo13-4

1.4313

 

S41500

F6NM

 

 

 

 

 

 

 

X4CrNiMo16-5-1

1.4418

 

 

 

 

248 SV

 

 

 

 

 

Martensitic and precipitation-hardening steels - special grades

X1CrNiMoCu12-5-2

1.4422

 

 

 

 

 

 

 

 

 

 

X1CrNiMoCu12-7-3

1.4423

 

 

 

 

 

 

 

 

 

 

X5CrNiCuNb16-4

1.4542

 

S17400

 

 

17-4 PH

 

 

 

 

 

X7CrNiAl17-7

1.4568

 

S17700

 

 

17-7 PH

 

AK

 

 

 

X10CrNi18-8

1.4310

301

S30100

 

301S21

 

ACE

 

 

 

 

X2CrNiN18-7

1.4318

301LN

S30153

 

 

 

 

 

 

OUT

 

X2CrNi18-9       

1.4307

304L

S30403

 

304S11

 

ACE

 

AP

OUT

 

X2CrNi19-11

1.4306

304L

S30403

 

 

 

 

 

 

OUT

 

X2CrNiN18-10

1.4311

304LN

S30453

 

304S51

 

 

 

 

OUT

 

X5CrNi18-10

1.4301

304

S30453

 

304S15

 

ACE

 

AP

OUT

 

X8CrNiS18-9

1.4305

303

S30300

 

303S31

 

 

 

 

 

 

X6CrNiTi18-10

1.4541

321

S32100

 

321S31

 

ACE

 

 

OUT

 

X4CrNi18-12

1.4303

305

S30500

 

305S19

 

 

 

 

 

 

X2CrNiMo17-12-2

1.4404

316L

S31603

 

316S11

 

ACE

 

AP

OUT

 

X2CrNiMoN17-11-2

1.4406

316LN

S31653

 

316S61

 

 

 

 

OUT

 

X5CrNiMo17-12-2

1.4401

316

S31600

 

316S31

 

ACE

 

 

OUT

 

X6CrNiMoTi17-12-2

1.4571

316Ti

S31635

 

320S31

 

ACE

 

 

OUT

 

X2CrNiMo17-12-3

1.4432

316L

S31603

 

316S13

 

ACE

 

 

OUT

 

X2CrNiMo18-14-3

1.4435

316L

S31603

 

316S13

 

 

 

 

OUT

 

X2CrNiMoN17-13-5

1.4439

317LMN

 

 

 

 

 

 

 

OUT

 

X1NiCrMoCu25-20-5

1.4539

 

N08904

 

904S13

904L

 

 

 

OUT

 

Austenitic stainless steels - special grades

X5CrNi17-7

1.4319

 

 

 

 

 

 

 

 

 

 

X5CrNiN19-9

1.4315

 

 

 

 

 

 

 

 

 

 

X5CrNiCu19-6-2

1.4640

 

 

 

 

 

 

 

 

 

 

X1CrNi25-21

1.4335

310L

 

 

 

 

 

 

 

 

 

X6CrNiNb18-10

1.4550

347

S34700

 

347S31

 

 

 

AP

 

 

X1CrNiMoN25-22-2

1.4466

310MoLN

S31050

 

 

 

 

 

 

 

 

X6CrNiMoNb17-12-2

1.4580

 

 

 

 

 

 

 

 

 

 

X2CrNiMoN17-3-3

1.4429

316LN

S31653

 

 

 

 

 

 

OUT

 

X3CrNiMo17-13-3

1.4436

316

S31600

 

316S33

 

 

 

 

OUT

 

X2CrNiMoN18-12-4

1.4434

317LN

S31753

 

 

 

 

 

 

 

 

X2CrNiMo18-15-4

1.4438

317L

 

 

317S12

 

 

 

 

OUT

 

X1CrNiMoCuN24-22-8

1.4652

 

 

 

 

 

 

 

 

OUT

 

X1CrNiSi18-15-4

1.4361

306

S30600

 

 

 

 

 

 

 

 

X11CrNiMnN19-8-6

1.4369

 

 

 

 

 

 

 

 

 

 

X6CrMnNiCuN18-12-4-2

1.4646

 

 

 

 

 

 

 

 

 

 

X12CrMnNiN17-7-5

1.4372

201

S20100

 

 

 

ACE

 

 

OUT

 

X2CrMnNiN17-7-5

1.4371

201L

S20103

 

 

 

 

 

AP

 

 

X9CrMnNiCu17-8-5-2

1.4618

 

 

 

 

 

 

 

AP

 

 

X12CrMnNiN18-9-5

1.4373

202

S20200

 

 

 

 

 

 

 

 

X9CrMnCuNB17-8-3

1.4597

204Cu

S20430

 

 

 

ACE

 

 

 

 

X8CrMnNi19-6-3

1.4376

 

 

 

 

 

 

 

 

 

 

X1NiCrMo31-27-4

1.4563

 

N08028

 

 

Sanicro 28

 

 

 

 

 

X1CrNiMoCuN25-25-5

1.4537

 

 

 

 

 

 

 

 

 

 

X1CrNiMoCuN20-18-7

1.4547

 

S31254

F44

 

254SMO

 

 

 

OUT

 

X1CrNiMoCuNW24-22-6

1.4659

 

 

 

 

 

 

 

 

 

 

X1NiCrMoCuN25-20-7

1.4529

 

N08925

 

 

1925hMo

 

 

 

OUT

 

X2CrNiMnMoN25-18-6-5

1.4565

 

 

 

 

 

 

 

 

OUT

 

X9CrMnNiCu 17-8-5-2

1.4618

 

 

 

 

 

 

 

AP

 

 

 

1.3964

 

 

 

 

Nitronic 50

 

 

 

 

 

Austenitic stainless steels - heat resisting grades

X8CrNiTi18-10

1.4878

321

S32100

 

 

 

ACE

 

 

OUT

 

X15CrNiSi20-12

1.4828

 

 

 

 

 

 

 

 

OUT

 

X9CrNiSiNCe21-11-2

1.4835

 

S30815

 

 

253 MA

 

 

 

OUT

 

X12CrNi23-13

1.4833

309

S30900

 

309S24

 

 

 

AP

OUT

 

X8CrNi25-21

1.4845

310S

S31000

 

310S24

153 MA

ACE

 

 

OUT

 

X15CrNiSi25-21

1.4841

314

S31400

 

 

330

 

 

 

OUT

 

X6CrNiSiNCe19-10

1.4818

 

S30415

 

 

 

 

 

 

OUT

 

X10NiCrSi35-19

1.4886

 

 

 

 

 

 

 

 

 

 

Austenitic stainless steels - creep resisting grades

X6CrNi18-10

1.4948

304H

S30409

 

304S51

 

 

 

 

 

 

X6CrNiMoB17-12-2

1.4919

304H

S31635

 

316S51

 

 

 

 

 

 

Austenitic-ferritic (Duplex) stainless steels - standard grades

X2CrNiN22-2

1.4062

 

S32202

 

 

 

 

 

AP

 

 

X2CrMnNiMoN21-5-3

1.4482

 

S32001

 

 

 

ACE

 

 

 

 

X2CrMnNiN21-5-1

1.4162

 

S32101

 

 

 

 

 

 

OUT

 

X2CrNiN23-4

1.4362

 

S32304

 

 

 

ACE

 

AP

OUT

 

X2CrNiMoN12-5-3

1.4462

 

S31803/

S32205

F51

318S13

2205

ACE

 

AP

OUT

 

Austenitic-ferritic (Duplex) stainless steels-special grades

X2CrNiCuN23-4

1.4655

 

 

 

 

 

 

 

 

 

 

X2CrNiMoN29-7-2

1.4477

 

 

 

 

 

 

 

 

 

 

X2CrNiMoCuN25-6-3

1.4507

 

 

F61

 

Ferrinox 255

 

 

 

 

 

X2CrNiMoN25-7-4

1.4410

 

S32750

F53

 

2507

 

 

AP

OUT

 

X2CrNiMoCuWN25-7-4

1.4501

 

S32760

F55

 

Zeron 100

 

 

 

 

NN

X2CrNiMoSi18-5-3

1.4424

 

 

 

 

 

 

 

 

 

 

 

Datasheets for Long Products Based on EN 10088-3

The table below contains all grades listed in EN 10088-3. In addition, there are some grades not in the current edition but which are expected to be in future editions. Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Some heat resisting steels from EN 10095 and creep resisting steels from EN 10302 are also included.

EN Designation Alternative designation
Steel name Steel number AISI UNS Other US BS Generic/Brand Datasheets
Ferritic stainless steels-standard grades
X2CrNi12 1.4003   S40977                
X6Cr13 1.4000 410S S41008   403S17            
X6Cr17 1.4016 430 S43000   430S17            
X6CrMoS17 1.4105 430F             Val    
X6CrMo17-1 1.4113 434 S43400                
Ferritic stainless steels-special grades
X2CrTi17 1.4520                    
X3CrNb17 1.4511                    
X2CrMoTiS18-2 4 1.4523                    
X6CrMoNb17-1 1.4526 436 S43600                
X2CrTiNb18 1.4509 441 S43932     18CrCb          
X2CrTi21 1.4611                    
X2CrNbCu21 1.4621                    
X2CrTi24 1.4613                    
Martensitic stainless steels-standard grades
X12Cr13 1.4006 410 S41000                
X12CrS13 1.4005 416 S41600                
X20Cr13 1.4021 420 S42000   420S29         Val  
X30Cr13 1.4028 420 S42000   420S45            
X39Cr13 1.4031 420 S42000   420S45            
X46Cr13 1.4034 420 S42000                
X38CrMo14 1.4419                    
X50CrMoV15 1.4116                    
X55CrMo14 1.4110                    
X14CrMoS17 1.4104                    
X39CrMo17-1 1.4122                    
X17CrNi16-2 1.4057 431 S43100   431S29           Smith
X3CrNiMo13-4 1.4313   S41500 F6NM              
X4CrNiMo16-5-1 1.4418         248SV          
Martensitic stainless steels-special grades
X29CrS13 1.4029                    
X46CrS13 1.4035                    
X70CrMo15 1.4109                    
X40CrMoVN16-2 1.4123                    
X105CrMo17 1.4125 440C S44004                
X90CrMoV18 1.4112 440B S44003                
X2CrNiMoV13-5-2 1.4415                    
X53CrSiMoVN16-2 1.4150                    
Martensitic stainless steels-creep resisting grades
X22CrMoV12-1 1.4923                    
Precipitation hardening stainless steels-standard grades
X5CrNiCuNb16-4 1.4542   S17400     17-4 PH  

 

     
X7CrNiAl17-7 1.4568   S17700     17-7 PH          
X5CrNiMoCuNb14-5 1.4594         FV 520B         Smith
Precipitation hardening stainless steels-special grades
X1CrNiMoAlTi12-9-2 1.4530                    
X1CrNiMoAlTi12-10-2 1.4596                    
X5NiCrTiMoVB25-12-2 1.4606                    
X1CrNiMoAlTi12-11-2 1.4612                    
Austenitic stainless steels-standard grades
X10CrNi18-8 1.4310 301 S30100   301S21            
X2CrNi18-9 1.4307 304L S30403   304S11            
X2CrNi19-11 1.4306 304L                  
X2CrNiN18-10 1.4311 304LN S30453                
X5CrNi18-10 1.4301 304 S30400   304S31            
X8CrNiS18-9 1.4305 303 S30300   303S31    

 

 

     
X6CrNiTi18-10 1.4541 321 S32100   321S31            
X4CrNi18-12 1.4303 305 S30500                
X2CrNiMo17-12-2 1.4404   S31603   316S11    

 

     
X2CrNiMoN17-11-2 1.4406 316LN                  
X5CrMo17-12-2 1.4401 316 S31600   316S31            
X6CrNiMoTi17-12-2 1.4571 316Ti     320S31            
X2CrNiMo17-12-3 1.4432 316L     316S13            
X2CrNiMoN17-13-3 1.4429 316LN                  
X3CrNiMo17-13-3 1.4436 316     316S33            
X2CrNiMo18-14-3 1.4435 316L                  
X2CrNiMoN17-13-5 1.4439                    
X6CrNiCuS18-9-2 1.4570                    
X3CrNiCu18-9-4 1.4567                    
X1NiCrMoCu25-20-5 1.4539                    
Austenitic stainless steels-special grades
X5CrNi17-7 1.4319 302               Ace  
X9CrNi18-9 1.4325                    
X5CrNiN19-9 1.4315                    
X6CrNiNb18-10 1.4550 347 S34700   347S31            
X1CrNiMoN25-22-2 1.4466 310MoLN S31050                
X6CrNiMoNb17-12-2 1.4580                    
X2CrNiMo18-15-4 1.4438 317L                  
X1CrNiMoCuN24-22-8 1.4652                    
X1CrNiSi18-15-4 1.4361                    
X11CrNiMnN19-8-6 1.4369                    
X13CrMnNiN18-13-2 1.4020                    
X6CrMnNiN18-13-3 1.4378                    
X6CrMnNiCuN18-12-4-2 1.4646                    
X12CrMnNiN17-7-5 1.4372 201 S20100                
X8CrMnNiN18-9-5 1.4374                    
X8CrMnCuNB17-8-3 1.4597                    
X3CrMnNiCu15-8-5-3 1.4615                    
X3CrNiCu19-9-2 1.4560                    
X3CrNiCuMo17-11-3-2 1.4578                    
X1NiCrMoCu31-27-4 1.4563                    
X1CrNiMoCuN25-25-5 1.4537                    
X1CrNiMoCuN20-18-7 4 1.4547   S31254     254 SMO         Smith
X2CrNiMoCuS17-10-2 1.4598                    
X1CrNiMoCuNW24-22-6 1.4659                    
X1NiCrMoCuN25-20-7 1.4529                    
X2CrNiMnMoN25-18-6-5 1.4565                    
  1.3964   S20910     Nitronic 50         Smith
      S21800     Nitronic 60         Smith
Austenitic stainless steels - Creep resisting steels
X6NiCrTiMoVB25-15-2 1.4980   S66286     A286          
Austenitic stainless steels - Heat resisting steels
X15CrNiSi20-12 1.4828                    
X9CrNiSiNCe21-11-2 1.4835   S30815     253 MA          
X8CrNi25-21 1.4845 310S S31008   310S31            
X15CrNiSi25-21 1.4841 314 S31400                
Austenitic-ferritic stainless steels-standard grades
X2CrNiN22-2 1.4062         DX 2202          
X2CrMnNiN21-5-1 1.4162   S32101     2101 LDX         Outo
X3CrNiMoN27-5-2 1.4460 329 S31260                
X2CrNiMoN22-5-3 1.4462  

S31803/

S32205

  318S13 2205          
Austenitic-ferritic stainless steels-special grades
X2CrNiN23-4 1.4362   S32304     2304          
X2CrMnNiMoN21-5-3 1.4482                    
X2CrNiMnMoCuN24-4-3-2 1.4662                   Outo
X2CrNiMoN29-7-2 4 1.4477                    
X2CrNiMoCuN25-6-3 1.4507   S32550     Ferrinox 255         Smith
X2CrNiMoN25-7-4 4 1.4410   S32750     2507         Smith
X2CrNiMoCuWN25-7-4 1.4501   S32760     Zeron 100          
X2CrNiMoSi18-5-3 1.4424                    

top

Office and Postal Address: BSSA, HQ, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital