Stainless Steel Grades Datasheets

Introduction

The Stainless Steel Advisory Service receives requests for datasheets for individual steel grades. Rather than create a new set of datasheets, it has been decided to make use of the excellent datasheets which already exist. These datasheets are most often linked to BSSA Members. Occasionally, we have included a datasheet for grades which are not covered by Members' datasheets.

Steel grades are arranged according to the main EN standards for flat and long products.

The codes used in the following tables are:

Ace Acerinox
AK AK Steel
AP Aperam
Out Outokumpu
Sm Smith Metal Centres
Val Valbruna

The existence of a datasheet for the more unusual grades probably indicates the ability to supply. However, the Special Grades Matrix gives a more comprehensive list of companies able to supply the product.

 Datasheets for Flat Products Based on EN 10088-2

The table below contains all grades listed in EN 10088-2. In addition, there are some grades not in the current edition but which are expected to be in future editions. Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Some heat resisting steels from EN 10095 and creep resisting steels from EN 10302 are also included.

EN Designation Alternative Designations  
Steel name Steel number AISI UNS Other US BS

Generic/Brand

Datasheets
Ferritic stainless steels - standard grades
X2CrNi12 1.4003   S40977     3CR12 AM   Outo Ace  
X2CrTi12 1.4512 409 S40900   409S19   AM   Outo Ace  
X6CrNiTi12 1.4516                    
X6Cr13 1.4000 410S S41008   403S17     AK      
X6CrAl13 1.4002 405 S40500   405S17            
X6Cr17 1.4016 430 S43000   430S17   AM   Outo Ace  
X3CrTi17 1.4510 439 S43035       AM   Outo Ace  
X3CrNb17 1.4511 430Nb               Ace  
X6CrMo17-1 1.4113 434 S43400   434S17         Ace  
X2CrMoTi18-2 1.4521 444 S44400       AM   Outo Ace  
Ferritic stainless steels - special grades
X2CrMnTi12 1.4600 - - - - -          
X2CrSiTi15 1.4630                    
X2CrTi17 1.4520                    
X1CrNb15 1.4595                    
X2CrMoTi17-1 1.4513           AM        
X6CrNi17-1 1.4017                    
X5CrNiMoTi15-2 1.4589   S42035                
X6CrMoNb17-1 1.4526 436 S43600       AM     Ace  
X2CrNbZr17 1.4590                    
X2CrTiNb18 1.4509 441 S43932     18CrCb AM   Outo Ace AK
X2CrNbTi20 1.4607                    
X2CrTi21 1.4611                    
X2CrTi24 1.4613                    
X2CrMoTi29-4 1.4592   S44700     29-4         All
X2CrNbCu21 1.4621   S44500       AM        
X2CrTiNbVCu22 1.4622   S44330           Outo    
Ferritic stainless steels - heat resisting grades
X10CrAlSi7 1.4713               Outo    
X10CrAlSi13 1.4724               Outo    
X10CrAlSi18 1.4742               Outo    
X18CrN28 1.4749 446                  
X10CrAlSi25 1.4762               Outo    
Martensitic stainless steels - standard grades
X12Cr13 1.4006 410 S41000   410S21            
X15Cr13 1.4024 420 S42000                
X20Cr13 1.4021 420 S42000   420S29   AM        
X30Cr13 1.4028 420 S42000   420S45   AM        
X39Cr13 1.4031 420 S42000   420S45         Ace  
X46Cr13 1.4034 420 S42000       AM        
X38CrMo14 1.4419           AM        
X55CrMo14 1.4110                    
X50CrMoV15 1.4116                 Ace  
X39CrMo17-1 1.4122                    
X3CrNiMo13-4 1.4313   S41500 F6NM              
X4CrNiMo16-5-1 1.4418         248 SV          
Martensitic and precipitation-hardening steels - special grades
X1CrNiMoCu12-5-2 1.4422                    
X1CrNiMoCu12-7-3 1.4423                    
X5CrNiCuNb16-4 1.4542   S17400     17-4 PH          
X7CrNiAl17-7 1.4568   S17700     17-7 PH         AK
Austenitic stainless steels - standard grades
X10CrNi18-8 1.4310 301 S30100   301S21         Ace  
X2CrNiN18-7 1.4318 301LN S30153           Outo    
X2CrNi18-9 1.4307 304L S30403   304S11   AM   Outo Ace  
X2CrNi19-11 1.4306 304L S30403           Outo    
X2CrNiN18-10 1.4311 304LN S30453   304S51       Outo    
X5CrNi18-10 1.4301 304 S30400   304S15   AM   Outo Ace  
X8CrNiS18-9 1.4305 303 S30300   303S31            
X6CrNiTi18-10 1.4541 321 S32100   321S31       Outo Ace  
X4CrNi18-12 1.4303 305 S30500   305S19       -    
X2CrNiMo17-12-2 1.4404 316L S31603   316S11   AM   Outo Ace  
X2CrNiMoN17-11-2 1.4406 316LN S31653   316S61       Outo    
X5CrNiMo17-12-2 1.4401 316 S31600   316S31       Outo Ace  
X6CrNiMoTi17-12-2 1.4571 316Ti S31635   320S31       Outo Ace  
X2CrNiMo17-12-3 1.4432 316L S31603   316S13       Outo Ace  
X2CrNiMo18-14-3 1.4435 316L S31603   316S13       Outo    
X2CrNiMoN17-13-5 1.4439 317LMN             Outo    
X1NiCrMoCu25-20-5 1.4539   N08904   904S13  904L     Outo    
Austenitic stainless steels - special grades
X5CrNi17-7 1.4319                    
X5CrNiN19-9 1.4315                    
X5CrNiCu19-6-2 1.4640                    
X1CrNi25-21 1.4335 310L                  
X6CrNiNb18-10 1.4550 347 S34700   347S31   AM        
X1CrNiMoN25-22-2 1.4466 310MoLN S31050                
X6CrNiMoNb17-12-2 1.4580                    
X2CrNiMoN17-3-3 1.4429 316LN S31653           Outo    
X3CrNiMo17-13-3 1.4436 316 S31600   316S33       Outo    
X2CrNiMoN18-12-4 1.4434 317LN S31753                
X2CrNiMo18-15-4 1.4438 317L     317S12       Outo    
X1CrNiMoCuN24-22-8 1.4652               Outo    
X1CrNiSi18-15-4 1.4361 306 S30600                
X11CrNiMnN19-8-6 1.4369                    
X6CrMnNiCuN18-12-4-2 1.4646                    
X12CrMnNiN17-7-5 1.4372 201 S20100           Outo Ace  
X2CrMnNiN17-7-5 1.4371 201L S20103       AM       All
X9CrMnNiCu17-8-5-2 1.4618           AM        
X12CrMnNiN18-9-5 1.4373 202 S20200                
X9CrMnCuNB17-8-3 1.4597 204Cu S20430             Ace  
X8CrMnNi19-6-3 1.4376                    
X1NiCrMo31-27-4 1.4563   N08028     Sanicro 28          
X1CrNiMoCuN25-25-5 1.4537                    
X1CrNiMoCuN20-18-7 1.4547   S31254 F44   254SMO     Outo    
X1CrNiMoCuNW24-22-6 1.4659                    
X1NiCrMoCuN25-20-7 1.4529   N08925     1925hMo     Outo    
X2CrNiMnMoN25-18-6-5 1.4565               Outo    
X9CrMnNiCu 17-8-5-2 1.4618           AM        
  1.3964         Nitronic 50          
Austenitic stainless steels - heat resisting Grades
X8CrNiTi18-10 1.4878 321 S32100           Outo Ace  
X15CrNiSi20-12 1.4828               Outo    
X9CrNiSiNCe21-11-2 1.4835   S30815     253 MA     Outo    
X12CrNi23-13 1.4833 309 S30900   309S24   AM   Outo    
X8CrNi25-21 1.4845 310S S31000   310S24       Outo Ace  
X15CrNiSi25-21 1.4841 314 S31400           Outo    
X6CrNiSiNCe19-10 1.4818   S30415     153 MA     Outo    
X10NiCrSi35-19 1.4886         330          
Austenitic stainless steels - creep resisting grades
X6CrNi18-10 1.4948 304H S30409   304S51            
X6CrNiMoB17-12-2 1.4919 316H S31635   316S51            
                       
                       
                       
Austenitic-ferritic stainless steels-standard grades
X2CrNiN22-2 1.4062   S32202     DX 2202 AM        
X2CrMnNiMoN21-5-3 1.4482   S32001             Ace  
X2CrMnNiN21-5-1 1.4162   S32101     2101 LDX     Outo    
X2CrNiN23-4 1.4362   S32304     2304 AM   Outo Ace  
X2CrNiMoN12-5-3 1.4462  

S31803/

S32205

 F51 318S13 2205 AM   Outo Ace  
Austenitic-ferritic stainless steels-special grades
X2CrNiCuN23-4 1.4655                    
X2CrNiMoN29-7-2 1.4477                    
X2CrNiMoCuN25-6-3 1.4507      F61   Ferrinox 255          
X2CrNiMoN25-7-4 1.4410   S32750  F53   2507 AM   Outo    
X2CrNiMoCuWN25-7-4 1.4501   S32760  F55   Zeron 100 RA        
X2CrNiMoSi18-5-3 1.4424                    

 

Datasheets for Long Products Based on EN 10088-3

The table below contains all grades listed in EN 10088-3. In addition, there are some grades not in the current edition but which are expected to be in future editions. Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Some heat resisting steels from EN 10095 and creep resisting steels from EN 10302 are also included.

EN Designation Alternative designation
Steel name Steel number AISI UNS Other US BS Generic/Brand Datasheets
Ferritic stainless steels-standard grades
X2CrNi12 1.4003   S40977                
X6Cr13 1.4000 410S S41008   403S17            
X6Cr17 1.4016 430 S43000   430S17            
X6CrMoS17 1.4105 430F             Val    
X6CrMo17-1 1.4113 434 S43400                
Ferritic stainless steels-special grades
X2CrTi17 1.4520                    
X3CrNb17 1.4511                    
X2CrMoTiS18-2 4 1.4523                    
X6CrMoNb17-1 1.4526 436 S43600                
X2CrTiNb18 1.4509 441 S43932     18CrCb          
X2CrTi21 1.4611                    
X2CrNbCu21 1.4621                    
X2CrTi24 1.4613                    
Martensitic stainless steels-standard grades
X12Cr13 1.4006 410 S41000                
X12CrS13 1.4005 416 S41600                
X20Cr13 1.4021 420 S42000   420S29         Val  
X30Cr13 1.4028 420 S42000   420S45            
X39Cr13 1.4031 420 S42000   420S45            
X46Cr13 1.4034 420 S42000                
X38CrMo14 1.4419                    
X50CrMoV15 1.4116                    
X55CrMo14 1.4110                    
X14CrMoS17 1.4104                    
X39CrMo17-1 1.4122                    
X17CrNi16-2 1.4057 431 S43100   431S29           Smith
X3CrNiMo13-4 1.4313   S41500 F6NM              
X4CrNiMo16-5-1 1.4418         248SV          
Martensitic stainless steels-special grades
X29CrS13 1.4029                    
X46CrS13 1.4035                    
X70CrMo15 1.4109                    
X40CrMoVN16-2 1.4123                    
X105CrMo17 1.4125 440C S44004                
X90CrMoV18 1.4112 440B S44003                
X2CrNiMoV13-5-2 1.4415                    
X53CrSiMoVN16-2 1.4150                    
Martensitic stainless steels-creep resisting grades
X22CrMoV12-1 1.4923                    
Precipitation hardening stainless steels-standard grades
X5CrNiCuNb16-4 1.4542   S17400     17-4 PH  

 

     
X7CrNiAl17-7 1.4568   S17700     17-7 PH          
X5CrNiMoCuNb14-5 1.4594         FV 520B         Smith
Precipitation hardening stainless steels-special grades
X1CrNiMoAlTi12-9-2 1.4530                    
X1CrNiMoAlTi12-10-2 1.4596                    
X5NiCrTiMoVB25-12-2 1.4606                    
X1CrNiMoAlTi12-11-2 1.4612                    
Austenitic stainless steels-standard grades
X10CrNi18-8 1.4310 301 S30100   301S21            
X2CrNi18-9 1.4307 304L S30403   304S11            
X2CrNi19-11 1.4306 304L                  
X2CrNiN18-10 1.4311 304LN S30453                
X5CrNi18-10 1.4301 304 S30400   304S31            
X8CrNiS18-9 1.4305 303 S30300   303S31    

 

 

     
X6CrNiTi18-10 1.4541 321 S32100   321S31            
X4CrNi18-12 1.4303 305 S30500                
X2CrNiMo17-12-2 1.4404   S31603   316S11    

 

     
X2CrNiMoN17-11-2 1.4406 316LN                  
X5CrMo17-12-2 1.4401 316 S31600   316S31            
X6CrNiMoTi17-12-2 1.4571 316Ti     320S31            
X2CrNiMo17-12-3 1.4432 316L     316S13            
X2CrNiMoN17-13-3 1.4429 316LN                  
X3CrNiMo17-13-3 1.4436 316     316S33            
X2CrNiMo18-14-3 1.4435 316L                  
X2CrNiMoN17-13-5 1.4439                    
X6CrNiCuS18-9-2 1.4570                    
X3CrNiCu18-9-4 1.4567                    
X1NiCrMoCu25-20-5 1.4539                    
Austenitic stainless steels-special grades
X5CrNi17-7 1.4319 302               Ace  
X9CrNi18-9 1.4325                    
X5CrNiN19-9 1.4315                    
X6CrNiNb18-10 1.4550 347 S34700   347S31            
X1CrNiMoN25-22-2 1.4466 310MoLN S31050                
X6CrNiMoNb17-12-2 1.4580                    
X2CrNiMo18-15-4 1.4438 317L                  
X1CrNiMoCuN24-22-8 1.4652                    
X1CrNiSi18-15-4 1.4361                    
X11CrNiMnN19-8-6 1.4369                    
X13CrMnNiN18-13-2 1.4020                    
X6CrMnNiN18-13-3 1.4378                    
X6CrMnNiCuN18-12-4-2 1.4646                    
X12CrMnNiN17-7-5 1.4372 201 S20100                
X8CrMnNiN18-9-5 1.4374                    
X8CrMnCuNB17-8-3 1.4597                    
X3CrMnNiCu15-8-5-3 1.4615                    
X3CrNiCu19-9-2 1.4560                    
X3CrNiCuMo17-11-3-2 1.4578                    
X1NiCrMoCu31-27-4 1.4563                    
X1CrNiMoCuN25-25-5 1.4537                    
X1CrNiMoCuN20-18-7 4 1.4547   S31254     254 SMO         Smith
X2CrNiMoCuS17-10-2 1.4598                    
X1CrNiMoCuNW24-22-6 1.4659                    
X1NiCrMoCuN25-20-7 1.4529                    
X2CrNiMnMoN25-18-6-5 1.4565                    
  1.3964   S20910     Nitronic 50         Smith
      S21800     Nitronic 60         Smith
Austenitic stainless steels - Creep resisting steels
X6NiCrTiMoVB25-15-2 1.4980   S66286     A286          
Austenitic stainless steels - Heat resisting steels
X15CrNiSi20-12 1.4828                    
X9CrNiSiNCe21-11-2 1.4835   S30815     253 MA          
X8CrNi25-21 1.4845 310S S31008   310S31            
X15CrNiSi25-21 1.4841 314 S31400                
Austenitic-ferritic stainless steels-standard grades
X2CrNiN22-2 1.4062         DX 2202          
X2CrMnNiN21-5-1 1.4162   S32101     2101 LDX         Outo
X3CrNiMoN27-5-2 1.4460 329 S31260                
X2CrNiMoN22-5-3 1.4462  

S31803/

S32205

  318S13 2205          
Austenitic-ferritic stainless steels-special grades
X2CrNiN23-4 1.4362   S32304     2304          
X2CrMnNiMoN21-5-3 1.4482                    
X2CrNiMnMoCuN24-4-3-2 1.4662                   Outo
X2CrNiMoN29-7-2 4 1.4477                    
X2CrNiMoCuN25-6-3 1.4507   S32550     Ferrinox 255         Smith
X2CrNiMoN25-7-4 4 1.4410   S32750     2507         Smith
X2CrNiMoCuWN25-7-4 1.4501   S32760     Zeron 100          
X2CrNiMoSi18-5-3 1.4424                    

top

Office and Postal Address: BSSA, HQ, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital