Related heat resisting stainless steel grades

Introduction

The table is intended to relate former BS, En, German and Swedish grade designations to the current EN steel numbers, AISI grades ('grades' in (brackets) are not a true AISI grades) and UNS (Unified Numbering System) numbers. The table is based on the 'wrought' ie long products (bars etc), flat products (plates etc) steel numbers published in EN 10095 and related standards. Castings products use different compositions and so have their own steel numbers in EN 10283. The related castings grades in both EN 10283 and BS 3100 are included in the table.

The 'Composition Guide' is intended to represent the composition only. This does not show the specified or typical compositions of commercially available steels. Specified ranges for the wrought European grades can be found in the BS EN 10095 table. Most of the specified ranges for the 'BS' grades can be found in the BS 1449 or BS 970 tables. The castings grades specified ranges can be found in the BS EN 10283 or BS 3100 tables. Direct links to tables giving the specified range is available for the grades with underlines in the table. Just click on the number.

As an alternative to scanning down the list try the 'find' facility on your keyboard, using the 'Ctrl' and 'F' keys together. Type in the term you are looking for in the dialog box that then appears.

These are comparisons only and cannot be assumed to be direct equivalent grades. The data given is not intended to replace that shown in individual standards to which reference should always be made.

Grades table

EN (10095) Common Names BS (Wrought) AISI UNS En German SS EN (10283) BS (Cast) Composition Guide
. . . . . . . . . . C Cr Ni Others
1.4713 Sicromal 8 - - - - X10CrAlSi7 - - - 0.12x 6 - 0.5Al
1.4724 - - - - - X10CrAl13 - - - 0.12x 12 - 1.0Al
1.4742 Sicromal 10 - - - - X10CrAl18 - - - 0.12x 17 - 1.0Al
1.4762 Sicromal 12 - - - - X10CrAl24 - - - 0.12x 23 - 1.5Al
1.4749 - - 446 S44600 - X18CrN28 - - - .15-.20 26 - 0.2N
1.4818 153MA - - S30415 - - 2371 - - .04-0.8 18 9 1.5Si:0.15N:0.05Ce
1.4828 - - - - - X15CrNiSi20-12 - - - 0.20x 19 11 2.0Si
1.4833 - 309S16 309 S30900 (S30908) - X12CrNi24-12 - - 309C30 0.15x 22 12 -
1.4835 253MA - - S30815 - X10CrNiSiN21-11 2368 - - .05-.12 20 10 2.0Si:0.15N:0.05Ce
1.4841 - - 314 S31400 - X15CrNiSi25-20 - - 310C45 0.20x 25 20 2.0Si
1.4845 - 310S24 310 S31000 (S31008) - X12CrNi25-21 - - - 0.10x 25 20 -
1.4854 353MA - - S35315 - X6NiCrSiNCe35-25 - - - 0.4-.08 25 35 1.5Si:0.15N:0.05Ce
1.4941 - 321S51 321H S32109 - X12CrNiTi18-9 2337 - - 0.10x 18 9 0.6Ti

Note
Composition Guide figures are intended to be representative of the grade, not typical.
'x' indicates a maximum

top

Office and Postal Address: BSSA, Regus, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2018 British Stainless Steel Association

web design sheffield by Llama Digital