  1. Ambient temperature mechanical properties of martensitic stainless steel flat products to BS EN 10088-2

    The BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 2014. Mechanical properties are specified, including proof and tensile strength, elongation, impact strength and hardness. Only tensile and hardness properties are tabulated in this article for the martensitic grades. LAST UPDATED 25th NOVEMBER 2014.

  2. Ambient temperature mechanical properties of precipitation hardening stainless steel flat products to BS EN 10088-2

    The BS EN 10088-2 is the material standard for stainless steel sheet, plate and strip for general purposes. The current edition was published in October 2014. Mechanical properties are specified include proof strength, tensile strength and elongation. These are tabulated in this article for the precipitation hardening grades 1.4542 and 1.4568. LAST UPDATED 25th NOVEMBER 2014.

  3. Ambient temperature mechanical properties of stainless steels to BS EN 10269

    BS EN 10269 is the material standard for stainless and heat-resisting steels, a selection of low alloy steels and some nickel alloys for fasteners. The ambient temperature mechanical properties shown in this article include 0.2% proof strength, tensile strength, elongation, reduction in area and impact (charpy) strength in the finally heat treated condition. Specified hardness levels for the steels for subsequent quenching and tempering (1.4923 1.4938 and 1.4913) in their delivery condition are also included.

  4. Ambient temperature physical properties of stainless steels to BS EN 10088-1

    Ambient temperature physical properties, including density, modulus of elasticity (Young's modulus), coefficient of thermal expansion, thermal conductivity, specific heat (heat content or heat capacity) and electrical resistivity for a range of ferritic, martensitic, austenitic and duplex stainless steel types are tabulated. Some explanation of the units used for these properties is given.

  5. American (ASTM) standards for stainless steels for general applications

    ASTM (American Society for Testing and Materials) standards are listed in sections covering flat and long products, tubes and pipes, forgings and castings in stainless steels. Standards listed include ASTM A450, A480, A484, A555, A167, A176, A666, A693, A276, A314, A493, A564, A565, A582, A182, A268, A269, A312, A358, A403, A409, A511, A554, A632, A731, A789, A790, A813, A814, A473, A705, A297, A743, A744 , A890, A999 and A1016. LAST REVIEWED 9th January 2012

  6. British and american standards for stainless steels for pressure vessel applications

    British and ASTM (American Society for Testing and Materials) standards are listed in sections covering flat and long products, tubes and pipes, forgings and castings in stainless steels. Standards listed include BSEN 10028-7, BS 1501-3, BSEN 10272, BS 1502, BS 3605, BSEN 10216-5, BSEN 10217-7, BS 3127, BSEN 10222-5, BS 1503, BSEN 10213-4, BS 1504, BS 4882, BSEN 10269, ASTM A240, A479, A336, A351 and A451. LAST REVIEWED 9th January 2012

  7. British and american standards for tolerances, surface finish and testing of stainless steels

    British and ASTM (American Society for Testing and Materials) standards are listed in sections covering tolerances, passivation and cleaning and testing products in stainless steels.  LAST REVIEWED 10th January 2012.

  8. British standards for stainless steels for general applications

    British standards are listed in sections covering flat and long products, tubes and pipes, forgings and castings in stainless steels. Standards listed include BSEN 10088, 10095, 10302, BS 1449, BSEN 10151, BS 970, BS 6258, BS 6744, BS 1554, BSEN 10270-3, BSEN 10263-5, BSEN 10090, (Valve Steels) BSEN 10312, BS 3059-2, BS 3606, BS 4127, BS4368-3, BS 4825, BS 5600-5, BS 6323-8, BS 6362, BS 7838, BSEN 1124, BSENISO 8752, BSENISO 9626, BSEN 10250-4, BSEN 10264-4, BSEN 10283, BS 3100, BS 3111-2, BS 3146-2 and BS MA29. LAST REVIEWED 10th January 2012.

  9. British standards for the welding and fabrication of stainless steels

    British standards are listed covering welding procedures and welding consumables, soldering and mechanical fasteners for stainless steels. Standards listed include BS 2633, BS 4677, BS 4515-2, BS 7475, BSEN 1011-3, BSEN 1600, BSEN 12072, BSEN 12073, BSEN 760, BSEN 287-1, BSEN 288, BS 6787, BS 5465, BSENISO 3506, BS6105 and BS 1210. LAST UPDATED 7th July 2004.

  10. BS 6744 2016 (May) Update - Stainless Steel Bars, Reinforcement of Concrete

    Stainless steel bars – Reinforcement of concrete – Requirements and test methods

    This European Standard specifies the requirements and test methods for solid stainless steel bars used for the reinforcement of concrete. It is applicable to ribbed stainless steel bars in grade 500. Several significant changes have been made to the earlier standard version i.e. BS6744:2001 + A2:2009, ‘Stainless steel bars for the reinforcement of and use in concrete – Requirements and test methods’ 

Page 3 of 14

  1. 1
  2. 2
  3. 3
  4. 4
  5. 5
  6. 6
  7. 7
  8. 8
  9. 9
  10. 10
  11. 11
  12. 12
  13. 13
  14. 14

top

Office and Postal Address: BSSA, Regus, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2017 British Stainless Steel Association

web design sheffield by Llama Digital