Trade names associated with stainless steels
Introduction
This list of trade names is for guidance only when trying to identify steel types from old or obscure drawings or specifications.
The list does not attempt to list the trade names of BSSA member companies, but some that crop-up frequently are included. BSSA member company product data should be obtained from their own literature or web-sites.
The list should not be considered to be totally comprehensive or complete. It is a historical listing and any contact details (company names and telephone numbers) given cannot be guaranteed to be current. No responsibility can be taken for its accuracy. Where shown, contact companies details may need to be rechecked.
Trade names table
Note, where 'Non-SS' is shown in the Nearest Grade column, this indicates that the trade name as not a stainless steel.
Use the 'Ctrl' and 'F' keys to 'find' a particular name.
| Trade Name | Nearest Grade | Description |
| 1925hMo | 1.4529 Austenitic | 20% chromium, 25% nickel, 6% molybdenum superaustenitic stainless steel (Krupp Thyssen Nirosta) |
| 2205 | 1.4462 Duplex | 22% chromium, 5% nickel, 3% molybdenum duplex stainless steel |
| 253MA | 1.4835 Heat Resisting | 21% chromium, 11% nickel, 1.5% silicon heat resisting stainless steel (AvestaPolarit) |
| 254SMO | 1.4547 Austenitic | 20% chromium, 18% nickel, 6% molybdenum superaustenitic stainless steel (AvestaPolarit) |
| 520B | 1.4594 Martensitic-PH | 13.5% chromium, 5.5% nickel, 1.5% molybdenum precipitation hardening grade |
| 904L | 1.4539 Austenitic | 20%chromium, 25% nickel, 4.5% molybdenum austenitic stainless steel |
| Abrazo | Non-SS | British Steel wear plates |
| Abro | Non-SS | Wear plates from James Fairley Abra Service Division 0121-327 7522 |
| Alencoflex | - | Flexible hoses with stainless steel braid outer covers from Alenco Hilyn, Enfield |
| Alloy 160 | 1.4713 | 1.4713 Heat resisting grade 7% Cr, Al - Bohler UK 0121-552 2575 - See Sicromal 8 |
| Aluchrom | - | VDM Trade Name for Fe-Cr alloys |
| Aquamet 22 | Nitronic 50 | Nitronic 50 type for propeller shaft applications - see Clements Engineering (St.Neots)Ltd for details |
| Armourcote | - | PTFE stainless composite coating for reducing friction from Armourcote Surface Treatments |
| Battle | - | Stainless steel holloware from GW Pearce, Birmingham |
| Brightray | Non-SS | Nickel alloys from Inco Alloys |
| Bundy | Non-SS | Brake pipe material from Armco also see Fulbraiz |
| Chemico | Non-SS | General purpose cleaner for stainless steel from The County Chemical Company, Birmingham 0121-744 2294 |
| Chichester | - | Stainless steel ware from Goodwood Metalcraft TEL 01243-784626 (also see Dexam International) |
| Colorcoat | Non-SS | Prepainted mild steel strip from British Steel (Corus Strip products) |
| Compass B555 | Non-SS | Wear plate with Brinell Hardness of 555HB - Sleema Engineers TEL 01922-408088 |
| Corrbloc | - | Mild steel strip clad with stainless steel |
| Corten A | Non-SS | Weathering steel from Corus Strip (British Steel) |
| Corten B | Non-SS | Weathering steel from Corus Plates (British Steel) |
| Cres | - | US military abbreviation for "Corrosion Resistant" implies any stainless steel ie not grade specific |
| Crominox | - | Aciers Crominox, Luxembourg now merged with Cromweld Steels as a 3Cr 12 supplier |
| Cromweld 3Cr12 | 1.4003 Ferritic | 3Cr12 ferritic stainless from Cromweld Steels, Stoke on Trent TEL 01782-374139 |
| Cronifer | - | Krupp VDM Trade Names for stainless steels |
| Cronix | - | Krupp VDM Trade Names for Ni-Cr heating element alloys |
| Cunifer | Non-SS | Krupp VDM Trade Names for copper-nickel alloys |
| Damac DL12 | Non-SS | Spot test paste supplied by Broadway Products |
| Delcrome | Non-SS | See Stellite - Product of Deloro Stellite, Swindon |
| Deloro | Non-SS | See Stellite - Product of Deloro Stellite, Swindon |
| Dessox | Non-SS | Oakite Ltd descaling compounds |
| Duranel | - | Clad plates involving combinations of stainless steel, aluminium and copper |
| Durasteel | Non-SS | Steel sheet with organic coating over zinc-nickel plated surface, originally from Japan (Nissan). Cape-Durasteel, Wellingborough TEL 01933-440555 |
| Durbar | 304, 316 | Floor or chequer plate - 304 & 316 now imported from Belgium (ALZ), stocked by Ancon CCL |
| Durehete | Non-SS | Heat resisting bar grades for bolting applications from Corus Engineering Steels, Rotherham |
| E-Brite 26-1 | - | Ferritic stainless steel with 26% Cr and extra low carbon (0.005% Max) from Airco Vacumetal, USA |
| EM 528 | - | Rolls Royce specification for 448 type turbine blade steel |
| Esshete | Non-SS | Heat resisting steel grades from Corus Engineering Steels |
| Ezeform | - | Patterned stainless steel strip from Atlas Steels, Canada for roofing applications |
| FAK 223 | 2205 | Also see "FALC 223" Duplex Stainless of a 2205 type from Krupp |
| FDP | 1.4541 Austenitic | "Firth's Decay Proof" (321) - see Firth Vickers 'Staybrite' |
| Fecralloy | - | Heat resistance wire, strip, bar grade 20% Cr, 5% Al,0.1% Y (yttrium) from Resistalloy, Sheffield TEL 0114-244 8634 |
| Ferralium 255 | 1.4507 Duplex | Superduplex stainless steel available from Langley Alloys Ltd, Newcastle-under-Lyme |
| Ferritescope | - | Magnetic permeability meter calibrated to show percentage of ferrite in austenitic stainless steels. from Fischer Instrumentation |
| Ferro-Di | - | Die casting process for stainless steel, GKN Crewe Technical Centre |
| FMB | 1.4401/1.4436 Austenitic | "Firth's Moly Bearing" (316, 2.25-3.0% Mo) - see Firth Vickers 'Staybrite' |
| Fliteline | - | PTFE flexible tubing with stainless steel braided wire sheathing for steam & water tubes from Unitubes, Slough TEL 01753-34931 |
| Genklene | Non-SS | Solvent containing trichloroethylene (not advised for health & environment reasons) |
| Hadfields Manganese Steel | Non-SS | Manganese steel, 12-14%Mn, for extreme wear resistant applications. Available from Corus Scunthorpe 01724-405779 Tim Peregrine |
| Hastelloy | Non-SS | Nickel based alloys |
| Haynes Alloys | Non-SS | Nickel based alloys, see Haynes Alloys brochures on shelf No2, cabinet No1 TEL 0161-223 5054 |
| Hexmetal | Non-SS | Armours for refractory linings from Causeway Steel Products, Gravesend TEL 01474-67871 |
| Hi-Proof | 316LN | Nitrogen bearing austenitics eg 316 bar for reinforcement, warm worked for 460 N/mm2 strength class |
| HR 3C | 310 | 25Cr - 20Ni - Nb - N variant of 310 as sulphurizing resistant grade from Sumitomo Metal Ind. |
| HWT | 430Ti | Hot Water Tank grade similar to 430Ti, with 19% Cr from Allegheny Ludlum |
| Hydroloy | - | Hydroloy HQ913 low erosion weld deposit austenitic grade available as weld deposit electrodes from Deloro Stellite |
| Hyform 409 | 1.4512 Ferritic | AvestaPolarit 409 type with titanium for automotive silencer tubing etc |
| Hyplus 29 | Non-SS | Corus Plates product |
| Hypress | Non-SS | C steel strip grade from Corus Strip Products, Brinsworth |
| Immac 5 | 1.4845 Heat Resisting | Heat resisting 310 (25 / 20) type originally a Firth Brown trade name |
| Immaculate V | - | Heat resisting 310 (25 / 20) with vanadium |
| IN744X | - | Microduplex superplastic experimental stainless steel |
| Incoclad | Non-SS | Nickel cladding alloys |
| Incoloy | Non-SS | Nickel heat resisting alloys (Incoloy DS 37Cr - 18Ni , Incoloy 800 same as Esshete 800) |
| Inconel | Non-SS | Nickel alloys |
| Inox | - | French (Spanish, Italian) general term for "stainless", not grade specific |
| Invar (Nilo 36) | Non-SS | Nickel alloy with 36% iron zero thermal expansion rate |
| Jethete | - | Martensitic stainless steel for aircraft turbine blades & engine casings |
| Kanthal | Non-SS | Heat Resistant & heating element alloys for furnace heating applications from Kanthal Ltd, Stoke on Trent TEL 01782-224800 |
| Kromar D70 | - | Cobalt containing stainless steel used for cluster bomblet flights made by Hunting Engineering. Believed to be an obsolete application. |
| Kunifer 10 | Non-SS | Brake pipe grade from Yorkshire Imperial Metals TEL 01532-701107 |
| M153D | - | Proprietary specification for a 316 free machining type with titanium additions type from IMI Witton |
| Macalloy | Non-SS | Reinforcement bar from Allied Steel & Wire (McCalls) TEL 0114-242 6704 |
| Meehanite | Non-SS | Cast Irons from The International Meehanite Metal Co, Reigate TEL 01737-244786 |
| MEK | Non-SS | Methylethyl ketone - solvent for removing plastic film & adhesives from stainless steel sheet |
| Meten 9 | 1.4828 Heat Resisting | Heat resisting stainless steel grade similar to Red Fox 34 from Mechanical Engineers, London |
| Monel | Non-SS | Nickel-copper alloys |
| Mu Metal | Non-SS | Alloy of 77% Ni,5% Cu, 4% Mo & Iron - Soft magnetic alloy with a high magnetic permeability |
| NACE | Non-SS | National Association of Corrosion Engineers (US) |
| Ni-Hard | Non-SS | Abrasion resistant castings 3.5/4.5 % Ni |
| Nichrome | Non-SS | Nickel Chromium heat resisting alloys for furnace heating elements |
| Nicorros | Non-SS | Nickel-copper alloys. |
| Nicrofer | Non-SS | VDM Trade Name for Ni-Cr-Fe & Ni-Cr-Fe-Mo alloys (TEL 01372-67137) - Nicrofer 3220=Incoloy 800,Nicrofer 3718=Incoloy DS,Nicrofer 4221=Incoloy 825,Nicrofer7216=Inconel 600,Nicrofer 7520=Nimonic75 |
| Nilo | Non-SS | Low expansion nickel alloy |
| Nimar | Non-SS | Maraging Steels from Corus Engineering Steels |
| Nimonic | Non-SS | Nickel based heat resisting eg Nimonic 75, 80, 90 |
| Niresist | Non-SS | Nickel cast iron from Lennox Foundry TEL 01322-383281 |
| Niroflex | - | Stainless steel safety clothing - CMT Industrial Supplies, Swansea 01792-798600 |
| Nirosta | - | Krupp Thyssen Nirosta (KTN) trade names for stainless steels, use Werkstoff numbers for grades eg "Nirosta 4301" as 1.4301 (304) |
| Nitralloy | Non-SS | Old ESC trade names for nitriding alloys En 41A & B, try Henry Whitham,Sheffield TEL 0114-244 0744 |
| Nitronic 50 | - | Also marketed as "Aquamet" |
| Novamet | Non-SS | Metal flakes from Hart Coating Technology TEL 01384-291513 |
| Nu Eli t | - | 18/2 ferritic stainless, titanium stabilized ferritic stainless (low interstitial) - old Nyby Uddeholm brands |
| Nu Monit | - | Titanium stabalised ferritic stainless (low interstitial) - old Nyby Uddeholm brands |
| Nuovinox | - | Aberneath Industries clad stainless bar products TEL 01639-820666 |
| Oztelloy | - | Stainless steel plating on various substrates - Tri-Kem Ltd Wellingborough - 01933-228877 |
| Pernifer | Non-SS | Krupp VDM Trade Names for 36% nickel-iron low expansion alloy |
| Planclad | - | Ductile Planetary Mill Ltd clad strip 304L, 430 & 410 stainless on carbon steel substrate |
| Polaris | Non-SS | Polaris stainless steel reviver (cleaner-polisher for table ware, sinks etc) - Dexam International |
| Poral | - | Porous sheet and strip (Pechiney Ugine Kulmann), not now available |
| Prodec | - | Avesta Sheffield free machining grades (Degerfors plate & bar) |
| Red Diamond | Non-SS | Wear resistant plates (Spartan Redheugh Ltd, Gateshead now closed) |
| Red Fox | - | Corus Engineering Steels Heat Resisting types RF310, RF309 & RF34 (RF34 also known as Meten 9 - 1.4828) |
| Regaflex | 316 | Flexible tube for flue linings in 316 type from Rega Metals Products |
| Remanit | - | Originally Thyssen trade name -- usually has werkstoff number added eg Remanit 4301 |
| Rigitube | - | Patterned tube for vehicle handrails (grab rails) - Rimex (Rigidized Metals) |
| Sanicro | - | Sandvik trade name eg Sanicro 28 (UNS N08028) |
| Sanmac | - | Sandvik improved machinability bar |
| Sea-Cure | 446 | Ferritic grade for seawater heat exchanger tubing- 26Cr, 3Mo, 2.5Ni UNS S44660 |
| Sicromal 10 | 1.4742 Heat Resisting | Heat resisting grade 17% Cr, AL - (Energy Alloys Rotherham 01709-788000) |
| Sicromal 12 | 1.4762 Heat Resisting | Heat resisting grade 24% Cr, Al - (Energy Alloys Rotherham 01709-788000) |
| Sicromal 8 | 1.4713 Heat Resisting | Heat resisting grade 7% Cr, Al - Bohler UK 0121-552 2575 as Alloy 160 or Energy Alloys Rotherham 01709-788000 |
| Silver Fox | - | Samuel Fox, later British Steel (Corus) Engineering Steels trade names |
| Sistema Men | - | Loose lay stainless steel floor tiles from Inova Furniture Contracts Ltd, London |
| Snaptite | - | Quick fitting couplings for fluid transfer lines in stainless steel with teflon seals from Adflow International Tel 01734-713733 |
| Sno-Trik | - | High-pressure stainless steel pipe fittings from Techmation Ltd (UK agents for Sno-Trik Co.) Tel "01-958 3111" |
| SS (41,400) | Non-SS | Japanese Structural Grades |
| St (37,52 etc) | Non-SS | German Structural Grades See BSEN 10025 |
| Staballoy | - | UNS S28200 - 17 Cr, 20 Mn 0.55 N |
| Staybrite | - | Generic trade names for Firth Vickers grades, such as FSL,FDP, FMB etc |
| Stavax | 420 | Tool steel type 0.38 C 13 Cr ie martensitic 420 type originally Uddeholm, later VEW Special Steels 0121-552 5681 |
| Steelex | 304,316 | Stainless steel roofing systems from Lee Steel Strip, Sheffield (now AvestaPolarit Strip) |
| Steelit | Non-SS | Complete Paint system for SS items from Stainless Steel Coatings Inc |
| Stellite | Non-SS | Cobalt hardfacing alloys - Deloro Stellite, Swindon TEL 01793-822451 |
| Stelvetite | Non-SS | Corus Strip plastic coated carbon steel strip products |
| Supatube | - | Welded SS Tube - weld bead drawn for hygienic & heat exchanger applications - Stelco Hardy, Treorchy |
| SuperDux 64 | - | Superplastic duplex stainless from Nippon Yakin Kigyo Co 25 Cr, 6.5 Ni, 3.2 Mo |
| Temet 25 | Nitronic 50 | Propeller shaft bar grade from Teignbridge Propellers Ltd, Newton Abbott TEL 01626-333377 FAX 01626-60783 |
| Thyroplast | - | Thyssen stainless steel generic trade name, Werksoff number used to identify specific grade |
| Triclad | - | Sandwich with mild steel core & stainless surfaces from Allegheny, USA - see Triply |
| Trinsul | - | Insulated profiled stainless steel sheet from Precision Metal Forming, Cheltenham 01242-527511 |
| Triply | - | Sandwich with mild steel core & stainless surfaces from Universal Cyclops, USA - see Triclad |
| Tufftriding | - | Salt bath nitrocarburising. Improves wear, seizure and galling resistance of 304 and 316 austenitic stainless steels, available from Keighley Laboratories Ltd. |
| Uginox | - | ArcelorMittal Stainless Europe trade names covering range of steel grades |
| UltiMet | - | 180 & 240 grit satin finishes from WS Metalstock Ltd |
| Uranus | - | Creusot Loire trade names examples Uranus B6, 50, 45N, 47 etc - stockist is James Fairley Athena |
| V2A | 304 | Krupp (Germany) trade names covering 304 types |
| V4A | 316 | Krupp (Germany) trade names covering 316 types |
| Waspalloy | Non-SS | Nickel-chromium alloys |
| Waukesha | Non-SS | Nickel alloy for anti-galling applications from Dewramet Ltd, Glasgow |
| Zalutite | Non-SS | AL, Zn Si coating on mild steel for car exhausts - Corus Strip Products |
| Zeron 100 | 1.4501 Duplex | Super duplex stainless steel (Rolled Alloys) |
| Zintec | Non-SS | Zinc coated mild steel from Corus Strip Products |

Follow us on Twitter