Stainless Steel Datasheets for Tubular Products
Introduction
The Stainless Steel Advisory Service receives requests for datasheets for individual steel grades. Rather than create a new set of datasheets, it has been decided to make use of the excellent datasheets which already exist. These datasheets are most often linked to BSSA Members. Occasionally, I have included a datasheet for grades which are not covered by Members' datasheets.
Steel grades are arranged according to the main EN standards for tubular products. The codes used in the following tables are:
| Aalco | Aalco |
| AM | Aperam |
| DMV | DMV |
| Out | Outokumpu |
| RA | Rolled Alloys |
| Sand | Sandvik |
The existence of a datasheet for the more unusual grades probably indicates the ability to supply. However, the Special Grades Matrix gives a more comprehensive list of companies able to supply the product.
Datasheets for Welded Tubes Based on EN 10296-2 and EN 10217-7
The table below contains all grades listed in EN 10296-2 (welded tubes for general purposes) and EN 10217-7 (welded tubes for pressure purposes). Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Grades in both standards are shown in bold. Grades only in EN 10296-2 are shown in normal. Grades only in EN 10217-7 are shown in italic.
| EN Designation | Alternative Designations | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Steel name | Steel number | AISI | UNS | Other US | BS |
Generic/Brand |
Datasheets | ||||
| Ferritic stainless steels | |||||||||||
| X2CrNi12 | 1.4003 | S40977 | 3CR12 | Aalco | AM | ||||||
| X2CrTi12 | 1.4512 | 409 | S40900 | 409S19 | AM | ||||||
| X6CrAl13 | 1.4002 | 405 | S40500 | 405S17 | |||||||
| X6Cr17 | 1.4016 | 430 | S43000 | 430S17 | AM | ||||||
| X3CrTi17 | 1.4510 | 439 | S43035 | AM | |||||||
| X2CrMoTi18-2 | 1.4521 | 444 | S44400 | AM | |||||||
| X6CrMoNb17-1 | 1.4526 | 436 | S43600 | AM | |||||||
| X2CrTiNb18 | 1.4509 | 441 | S43932 | 18CrCb | AM | ||||||
| Austenitic stainless steels | |||||||||||
| X2CrNiN18-7 | 1.4318 | 301LN | S30153 | ||||||||
| X2CrNi18-9 | 1.4307 | 304L | S30403 | 304S11 | AM | ||||||
| X2CrNi19-11 | 1.4306 | 304L | S30403 | AM | |||||||
| X2CrNiN18-10 | 1.4311 | 304LN | S30453 | 304S51 | |||||||
| X5CrNi18-10 | 1.4301 | 304 | S30400 | 304S15 | AM | ||||||
| X6CrNiTi18-10 | 1.4541 | 321 | S32100 | 321S31 | AM | ||||||
| X6CrNiNb18-10 | 1.4550 | 347 | S34700 | 347S31 | - | ||||||
| X2CrNiMo17-12-2 | 1.4404 | 316L | S31603 | 316S11 | AM | ||||||
| X5CrNiMo17-12-2 | 1.4401 | 316 | S31600 | 316S31 | AM | ||||||
| X6CrNiMoTi17-12-2 | 1.4571 | 316Ti | S31635 | 320S31 | AM | ||||||
| X2CrNiMo17-12-3 | 1.4432 | 316L | S31603 | 316S13 | |||||||
| X2CrNiMoN17-3-3 | 1.4429 | 316LN | S31653 | ||||||||
| X3CrNiMo17-13-3 | 1.4436 | 316 | S31600 | 316S33 | |||||||
| X2CrNiMo18-14-3 | 1.4435 | 316L | S31603 | 316S13 | |||||||
| X2CrNiMoN17-13-5 | 1.4439 | 317LMN | S31726 | But | |||||||
| X1NiCrMoCu25-20-5 | 1.4539 | N08904 | 904S13 | 904L | Outo | ||||||
| X1CrNiMoCuN20-18-7 | 1.4547 | S31254 | F44 | 254SMO | Outo | ||||||
| X6CrNiMoNb17-12-2 | 1.4580 | S31640 | |||||||||
| X2CrNiMo18-15-4 | 1.4438 | 317L | S31703 | 317S12 | |||||||
| X1CrNiMoCuN24-22-8 | 1.4652 | S32654 | 654SMO | Outo | |||||||
| X1NiCrMo31-27-4 | 1.4563 | N08028 | Sanicro 28 | But | |||||||
| X1CrNiMoCuN25-25-5 | 1.4537 | N08932 | |||||||||
| X1CrNiMoCuNW24-22-6 | 1.4659 | S31266 | |||||||||
| X1NiCrMoCuN25-20-7 | 1.4529 | N08925 | 1925hMo | But | |||||||
| Austenitic stainless steels - heat resisting Grades | |||||||||||
| X15CrNiSi20-12 | 1.4828 | AM | |||||||||
| X9CrNiSiNCe21-11-2 | 1.4835 | S30815 | 253 MA | RA | |||||||
| X12CrNi23-13 | 1.4833 | 309 | S30900 | 309S24 | AM | RA | |||||
| X8CrNi25-21 | 1.4845 | 310S | S31000 | 310S24 | RA | ||||||
| X6CrNiSiNCe19-10 | 1.4818 | S30415 | 153 MA | Outo | |||||||
| X6NiCrSiNCe35-25 | 1.4854 | S35315 | 353MA | ||||||||
| X10NiCrSi35-19 | 1.4886 | N08330 | 330 | RA | |||||||
| Austenitic-ferritic stainless steels | |||||||||||
| X2CrMnNiN21-5-1 | 1.4162 | S32101 | 2101 LDX | Outo | |||||||
| X2CrNiN23-4 | 1.4362 | S32304 | 2304 | Outo | |||||||
| X2CrNiMoN12-5-3 | 1.4462 |
S31803/ S32205 |
F51 | 2205 | Outo | RA | |||||
| X2CrNiMoN25-7-4 | 1.4410 | S32750 | F53 | 2507 | Outo | ||||||
| X2CrNiMoCuEWN25-7-4 | 1.4501 | S32760 | F55 | Zeron 100 | RA | ||||||
Datasheets for Seamless Tube Products Based on EN 10297-2 and EN 10216-5
The table below contains all grades listed in EN 10297-2 (seamless tubes for general purposes) and EN 10216-5 (seamless tubes for pressure purposes). Not all grades can be linked to a datasheet. This reflects the apparent fact that some steels in the Standard are not practically available. Grades in both standards are shown in bold. Grades only in EN 10297-2 are shown in normal. Grades only in EN 10216-5 are shown in italic.
| EN Designation | Alternative designation | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Steel name | Steel number | AISI | UNS | Other US | BS | Generic/Brand | Datasheets | |||||
| Ferritic stainless steels | ||||||||||||
| X2CrTi12 | 1.4512 | 409 | S40900 | 409S19 | ||||||||
| X6CrAl13 | 1.4002 | 405 | S40500 | 405S17 | ||||||||
| X6Cr17 | 1.4016 | 430 | S43000 | 430S17 | ||||||||
| X3CrTi17 | 1.4510 | 439 | S43035 | |||||||||
| Martensitic stainless steels | ||||||||||||
| X12Cr13 | 1.4006 | 410 | S41000 | |||||||||
| Austenitic stainless steels | ||||||||||||
| X2CrNi18-9 | 1.4307 | 304L | S30403 | 304S11 | ||||||||
| X2CrNi19-11 | 1.4306 | 304L | S30403 | |||||||||
| X2CrNiN18-10 | 1.4311 | 304LN | S30453 | |||||||||
| X5CrNi18-10 | 1.4301 | 304 | S30400 | 304S31 | ||||||||
| X8CrNiS18-9 | 1.4305 | 303 | S30300 | 303S31 |
|
|||||||
| X6CrNiTi18-10 | 1.4541 | 321 | S32100 | 321S31 | ||||||||
| X6CrNiNb18-10 | 1.4550 | 347 | S34700 | 347S31 | ||||||||
| X1CrNi25-21 | 1.4335 | 310L | S31002 | Sand | ||||||||
| X2CrNiMo17-12-2 | 1.4404 | S31603 | 316S11 |
|
||||||||
| X5CrMo17-12-2 | 1.4401 | 316 | S31600 | 316S31 | ||||||||
| X1CrNiMoN25-22-2 | 1.4466 | 310MoLN | S31050 | DMV | Sand | |||||||
| X6CrNiMoTi17-12-2 | 1.4571 | 316Ti | S31635 | 320S31 | ||||||||
| X6CrNiMoNb17-12-2 | 1.4580 | S31640 | ||||||||||
| X2CrNiMoN17-13-3 | 1.4429 | 316LN | S31653 | |||||||||
| X3CrNiMo17-13-3 | 1.4436 | 316 | S31600 | 316S33 | ||||||||
| X2CrNiMo18-14-3 | 1.4435 | 316L | S31603 | DMV | Sand | |||||||
| X2CrNiMoN17-13-5 | 1.4439 | S31703 | ||||||||||
| X1NiCrMoCu31-27-4 | 1.4563 | N08028 | Sanicro 28 | Sand | ||||||||
| X1NiCrMoCu25-20-5 | 1.4539 | N08904 | 904L | Sand | ||||||||
| X1CrNiMoCuN20-18-7 4 | 1.4547 | S31254 | 254 SMO | Sand | ||||||||
| X1NiCrMoCuN25-20-7 | 1.4529 | N08925 | ||||||||||
| X2NiCrAlTi32-20 | 1.4558 | N08800 | Sand | |||||||||
| Ferritic heat resisting steels | ||||||||||||
| X18CrN28 | 1.4749 | S44600 | Sand | |||||||||
| Austenitic heat resisting steels | ||||||||||||
| X8CrNiTi18-10 | 1.4878 | 321 | S32109 | |||||||||
| X9CrNiSiNCe21-11-2 | 1.4835 | S30815 | 253 MA | Sand | ||||||||
| X12CrNi23-13 | 1.4833 | S30900 | 309S24 | Sand | ||||||||
| X8CrNi25-21 | 1.4845 | 310S | S31008 | 310S31 | Sand | |||||||
| X10NiCrAlTi32-21 | 1.4876 | N08810 | ||||||||||
| X6NiCrSiNCe35-25 | 1.4854 | S35315 | Sand | |||||||||
| X10NiCrSi35-19 | 1.4886 | N08330 | 330 | RA | ||||||||
| Austenitic creep resisting steels | ||||||||||||
| X6CrNi18-10 | 1.4948 | 304H | ||||||||||
| X7CrNiTi18-10 | 1.4940 | 321H | ||||||||||
| X7CrNiNb18-10 | 1.4912 | 347H | ||||||||||
| X6CrNiTiB18-10 | 1.4941 | 321H | ||||||||||
| X6CrNiMo17-13-2 | 1.4918 | 316N | Sand | |||||||||
| X5NiCrAlT31-20 | 1.4958 | |||||||||||
| X8CrNiAlTi32-21 | 1.4959 | Sand | ||||||||||
| X3CrNiMoBN17-13-3 | 1.4910 | 316LN | ||||||||||
| X8CrNiNb16-13 | 1.4961 | |||||||||||
| X8CrNiMoVNb16-13 | 1.4988 | |||||||||||
| X8CrNiMoNb16-16 | 1.4981 | |||||||||||
| X10CrNiMoMnNbVB15-10-1 | 1.4982 | Sand | ||||||||||
| Austenitic-ferritic stainless steels | ||||||||||||
| X2CrNiN23-4 | 1.4362 | S32304 | 2304 | Sand | ||||||||
| X3CrNiMoN27-5-2 | 1.4460 | 329 | S31260 | Sand | ||||||||
| X2CrNiMoN29-7-2 4 | 1.4477 | |||||||||||
| X2CrNiMoN22-5-3 | 1.4462 |
S31803/ S32205 |
2205 | DMV | Sand | |||||||
| X2CrNiMoCuN25-6-3 | 1.4507 | S32550 | Ferrinox 255 | DMV | ||||||||
| X2CrNiMoN25-7-4 4 | 1.4410 | S32750 | 2507 | Sand | ||||||||
| X2CrNiMoCuWN25-7-4 | 1.4501 | S32760 | Zeron 100 | DMV | ||||||||
| X2CrNiMoSi18-5-3 | 1.4424 | S31500 | Sand | |||||||||