Baffle Curtains? Stainless UK Provide the Solution

15 Sep 2014

Stainless UK has supplied 4 custom made stainless steel baffle curtains to contractor Acrefield Developments for use as part of a major refurbishment of Grange Service Reservoir in the Wirral.

 

The rigid baffle curtains in heights of up to 7.5m were manufactured from marine Grade 316 stainless steel sheet in Stainless UK’s Sheffield factory. They were used to form partition walls in the reservoir tank in conjunction with Acrefield’s flexible protective membrane baffle system. Due to the complex shape of the tank, each baffle curtain had to be made to an individual design. In addition to the panels, Stainless UK also manufactured custom made support beams, brackets, access doors and supplied all the fixings to install the system.

 

Once the specifications had been agreed, Stainless UK had to work to a tight delivery schedule for the baffles due to the limited window of access to site. Work started in April and was completed on time in June.

 

Stainless UK has been supplying the water industry for over 20 years with made to order stainless steel products ranging from ladders and platforms to tie bar systems for sewage tanks.

 

For further information please contact Tony Rice at Stainless UK Ltd on: tony@stainless-uk.co.uk or call +44 (0)114 244 1333

www.stainless-uk.co.uk

 


top

Office and Postal Address: BSSA, Regus, Blades Enterprise Centre, John Street, Sheffield S2 4SW

Registered Office: Pegasus House, 463A Glossop Road, Sheffield S10 2QD

Tel: +44 (0)114 292 2636    |     Email: admin@bssa.org.uk

Copyright © 2017 British Stainless Steel Association

web design sheffield by Llama Digital