Structural Design of Ferritic Stainless Steels

09 Jun 2014

The SCI guide Structural Design of Ferritic Stainless Steels complements the existing guidance on austenitic and duplex stainless steels. The 3 year progamme was carried out under the EU's Research Fund for Coal and Steel. Design guidance has been developed for a number of ferritic stainless steel grades including:

 

1.4003, 1.4016 (430), 1.4509 (441), 1.4621 (445), 1.4521 (444)

 

The full content of the report and detailed work packages can be found at www.steel-stainless.org/ferritics.

 