Contact BSSA

Flat Products - Stainless Steel Stocks Rise

30 Apr 2014

According to statistics released by Eurofer, stock levels have been rising in Western Continental Europe (i.e. excluding the UK).

 

Using a measure of “Calendar Days of Coverage” stock days have risen for the three months of December, January and February to a level of 61 days. This though is still considerably below the pre-crash level in 2008 of circa 85 days.

 

We will update this statistic once further reports are filed.