Barnshaw Section Benders were awarded the Al Emaan Mosque bending work this January. The job contracted by company App Steel Structures involved Barnshaws experts forming the main frame ribs and curving the support steelwork in 2 planes (canted).

Barnshaws benders received the structural project due to excellent technical expertise of ‘canting’ the 100 x 60 RHS and mandrel forming of 200 x 100 RHS to minimize distortion.

Barnshaws supplied the mosque with 200 x 100 x 6.3 RHS and 100 x 60 x 3 RHS, which were approximately 4 tonnes.